Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market (2015) of $33 billion, lead acid is the most common battery in use. This is followed by Li-ion at $16.6 billion, NiMH at $2 billion and NiCd at $1 billion. All other chemistries only make up $1 billion. Table 1 lists the material cost per ton to build these batteries.

Battery Chemistry Metal Value (per ton)* Recycling
Lithium cobalt oxide $25,000

Subsidy needed

Cobalt $50,000 Relevant, subsidy
Lithium iron phosphate $400

Subsidy needed

Lead acid $1,500 Profitable
Nickel$10,000–$17,000Subsidy needed
Cadmium$2,200Subsidy needed
Table 1: Metal value per ton of battery
Lead acid remains the most suitable battery to recycle; 70% of its weight contains reusable lead.
* 2017 Reference prices only; purity and supply govern value.

Lithium-ion batteries are expensive to manufacture and this is in part due to the high material cost and complex preparation processes. The most expensive metal of most Li-ion is cobalt, a hard lustrous gray material that is also used to manufacture magnets and high-strength alloys.

Knowing that billions of Li-ion batteries are discarded every year and given the high cost of lithium cobalt oxide, salvaging precious metals should make economic sense and one wonders why so few companies recycle these batteries.

The reason becomes clear when examining the complexity and low yield of recycling. The retrieved raw material barely pays for labor, which includes collection, transport, sorting into batteries chemistries, shredding, separation of metallic and non-metallic materials, neutralizing hazardous substances, smelting, and purification of the recovered metals.

Lead Acid

Recycling programs for lead acid are said to have started soon after Cadillac introduced the cranking motor in 1912 as a for-profit business rather than protecting the environment. Recycling can be harmful, especially with lead acid batteries. Lead can enter the body by inhaling or ingestion when touching the mouth with lead-contaminated hands. This puts workers and residents of the surrounding areas at risk of lead poisoning. (See BU-703: Health Concerns with Batteries)

The EPA (Environmental Protection Agency) has imposed strict guidelines in recycling of lead acid batteries in the USA. The recycling plants must be sealed and the smokestacks fitted with scrubbers. To check for possible escape of lead particles, the plant perimeter must be surrounded with lead-monitoring devices. Rules are bound to be broken and batteries soon end up in Mexico and other developing countries with relaxed regulations. China, a leader in lead acid battery production, also took action to protect the environment by introducing strict guidelines that only reputable companies can meet.

Nickel

Nickel-based batteries can also be recycled and the retrieved materials are iron and nickel, which are used in stainless steel production. Nickel-metal-hydride (NiMH) yields the highest return in nickel, and with ample supply recycling is said to make money. Low demand for cadmium has reduced the profitability from recycling NiCd batteries. The growth in batteries is with Li-ion but valuable materials are difficult to retrieve. This makes Li-ion less attractive for recycling and a financial breakeven may not be possible without subsidies.

Li-ion

The true cost to manufacture Li-ion is not so much in the raw materials, as is the case with lead acid and NiMH, but in lengthy processing and purification processes of the raw materials to reach battery grade. Retrieving lithium at only 3 percent of the cell mix may never reach break-even levels. If the purity of lithium is below 99.5 percent, then it is not suitable as raw material for batteries. Recycling brings the metal to ground zero, from which costly preparations begin anew. It is often cheaper to mine raw material than to retrieve it from recycling. Lithium from recycled batteries is commonly used for non-battery applications, such as lubricating greases that are found in WD-40 and other products, rather than batteries. (See BU-308: Availability of Lithium)

Direct recycling technologies for lithium-ion batteries my offer a solution in refining used Li-ion into high value cathode and anode materials. Direct recycling may become profitable if the technology can be developed to large-scale processing made possible with high volume EV batteries reaching end-of-life. Direct recycling is said to be cleaner than older methods that melt the material.

Alkaline

Although alkaline and zinc-carbon account for over 90 percent of batteries consumed in the United States, they contain few precious metals and the toxicity is low. Organizations are seeking ways to recycle these batteries as well for the basic metal content and with high volume such a venture should become viable. Table 2 lists the typical metals content of commonly recycled batteries.

Fe
Iron
Mn
Manganese
Ni
Nickel
Zn
Zinc
Li
Lithium
Cd
Cadmium
Co
Cobalt
Al
Aluminum
Pb
Lead
Lead acid
65%
NiCd
35%
22%

15%
NiMH
20%
1%
35%
1%

4%
Li-ion
22%



3%
18%
5%
Alkaline
24%
22%
15%
Table 2: Metals in commonly recycled batteries as a percentage of the overall content
The metal content may vary with battery type. With the exception of lead acid, most recycling requires a subsidy.

Facts about Battery Production and Recycling

Environmental issues and the ability to recycle play an important role when choosing a battery system. If the UPS operates mostly in standby and can provide longevity of 10 years, then lead acid is a strong contender. The preference of lead acid over Li-ion and nickel-based systems is manifested in moderate pricing, superior safety, dependable operation, and the ability to recycle. Table 3 compares the cost to manufacture and recycle batteries.


Estimated Cost of Disposal Production Process Carbon Dioxide Emission
Lead acid Profitable; lead has intrinsic value 30 mega joules; 8.3kW* 3kg per kg*
Lithium-ion $4,000–5,000 per ton 170 mega joules; 47kW* 12kg per kg*
NiCd, NiMH Can be cost neutral N/A N/A
Table 3: Costs of battery manufacturing and disposal
* Quoted figures from Argonne National Laboratory

Summary

The primary objective of building a good battery is long life, safety and low price. Recycling is an afterthought and manufacturers do little to simplify the retrieving of precious metals. The recycling business is small compared to the vast battery industry, and to this day, only lead acid can be recycled profitably.

Nickel-based batteries might make money with good logistics, but Li-ion and most other chemistries yield too little in precious metals to make recycling a viable business without subsidies. The major expense with modern batteries is not so much the raw materials, as with lead acid, but lengthy preparations, purifications and processing down to micro- and nano-levels. Nevertheless, batteries contain valuable material that can be re-used for new products.

To make recycling feasible in the meantime, subsidies are created by adding a tax to each pack sold. The goal goes beyond retrieving metals for re-use to preventing toxic batteries from entering landfills. Combining the environmental benefit with making a profit is the ultimate goal, and this might become feasible with innovative new recycling processes in development.

Another model is to sort batteries into functional and non-functional groups and give those with capacities of 80 percent or more a second life. Cells and modules of larger battery systems can be tested individually and reassembled in a new pack(See BU-803: Can Batteries be Restored?)

Last Updated: 29-Oct-2021
Batteries In A Portable World
Batteries In A Portable World

The material on Battery University is based on the indispensable new 4th edition of "Batteries in a Portable World - A Handbook on Rechargeable Batteries for Non-Engineers" which is available for order through Amazon.com.

Comments

Comments are intended for "commenting," an open discussion amongst site visitors. Battery University monitors the comments and understands the importance of expressing perspectives and opinions in a shared forum. However, all communication must be done with the use of appropriate language and the avoidance of spam and discrimination.

If you have a suggestion or would like to report an error, please use the "contact us" form or email us at: BatteryU@cadex.com. We like to hear from you but we cannot answer all inquiries. We recommend posting your question in the comment sections for the Battery University Group (BUG) to share.

I understand. Hide this message.
Looking for comments from the previous website?

Comments from the previous website are not compatible with our new commenting system but we have preserved them so our users can still reference and make use the information in them.

Show Old Comments
On July 26, 2019, Mohd Rashid wrote:
Thanks for the reply. Mr Jane @ Darius My company is in India Yes my company can supply 250,000 Lithium batteries. We have also removed anode & cathode foil from the case.Which is about 50 Tons E-mail; arkrashid20@gmail.com Mobile; 91-7550633477
On July 25, 2019, jane wrote:
@ Darius are you selling your batteries? My company is looking to purchase up to 250,000 lithium batteries. Please email me with your information. Thank you
On July 12, 2019, Mohd Rashid wrote:
We are selling our stock of anode & cathode foils of spent Li-ion & lap-top batteries. Our stock is more than 40 metric tons
On July 8, 2019, Vikas tomar wrote:
Our objective is to set-up a large capaity LEAD BATTERY RECYCLE PLANT, as replica of & with associated Korean company, which has quickened, pointing to a time of age attracted the advanced technology of extra alloy metal the first of the industries of recycling lead and remelting in domestic, and completed the factory whose capacity is 6,000 ton monthly of alloy lead. Preference is to set-up plant in north India in a approved Industrial land area of min. of 4 acr or 12,200 Sq Mtr.,scalable to total of 5 Acr or 20,200 Sq. Mtr. I want to source large quantity of Lead Recycley Battery, in a magnitude of 10,000 Tonns a month on an anualaized contract.
On June 20, 2019, darius wrote:
Jane Gallagher , I have 50 x 90Ah used lithium phosphate batteries from electric car (loco Europe) make: Headway BTW Ask https://batteryuniversity.com/index.php/learn/article/battery_recycling_as_a_business to update data on pricing of metals Battery Chemistry Metal value (per ton) Recycling Table 1: Metal value per ton of battery. Lead acid remains the most suitable battery to recycle; 70% of its weight contains reusable lead. Lithium cobalt oxide $25,000 Subsidy needed Cobalt $50,000 (2017) Relevant, subsidy Lithium iron phosphate $400 Subsidy needed Lead acid $1,500 Profitable Nickel $10,000–$17,000 Subsidy needed Cadmium $2,200 Subsidy needed being as old as of 2015
On June 19, 2019, Jane Gallagher wrote:
Hi all. I am looking to buy used lithium phosphate batteries. Can anyone point me in the right direction or know of anywhere that is selling them ? Thank you, I welcome any information, please email jgallagher@autocruisint.com
On June 12, 2019, Jeff SEO wrote:
Hi all? We are located in South Korea and we have ready to move stock of new, used and scrap Li-ion, Li-Polymer batteries that can be sourced on a regular basis. Anyone interested, please contact us at jnbco@gmail.com or WhatsApp +821090775280. Thank you.
On February 3, 2019, Alethinos wrote:
We are just going into lead battery recycling business in Nigeria.We need a business partner that will provide the equipment and we want to assure you that Nigeria environment is highly conclusive for battery business since the raw material is in abundant The prospective investor is expected to source for off takers in overseas countries. Any interested investor can please contact me through my e mail address alethinossb@gmail.com.+2348180780098
On January 4, 2019, MOHD RASHID wrote:
Require in bulk quantity spent mobile Lithium ion batteries for Recycling. Please contact; 91-7550633477 e-mail; arkrashid20@gmail.com
On December 15, 2018, vikas patnaik wrote:
hello startups Am here a consultant and manufacturer For making lead batteries and solar panels Like E rickshaw batteries Two Wheeler batteries Inverters batteries solar panels For any information contact me But pls don’t waste time of mine and your self by calling me as a fake . Thank you Vikas patnaik S&B.UC {Solar and Battery unit consultant} consultant for battery unit setup and solar power unit setup Business phone no. +91 7027891346 Business gmail id : vikaspatnaik77@gmail.com Professional linkedin id : vikas patnaik. (entrepreneur investor and CEO at vigorous) Website : search vigorous batteries
On October 30, 2018, Tiger wrote:
we buy end of life mobile and laptop batteries. kindly whatsapp +.+919082598288
On October 29, 2018, serjo wrote:
I'm looking for a buyer of lithium batteries from the cellular industry. My company is located in South America. Be happy to get details from you Thanks in advance email :serjo.vh@gmail.com whatsapp : +972545833004
On September 29, 2018, Kolapo Ayoola RAJI wrote:
I am just going into battery recycling business in Nigeria . I need a business partner that will provide the equipment and I want to assure you that Nigeria environment is highly conclusive for battery business since the raw material is in abundant The prospective investor is expected to source for off takers in overseas countries Any interested investor can please contact me through my e mail address
On September 22, 2018, Sierra metals recycling wrote:
Fatima Susana Martinez Lopez, Hi we are a battery recycling company based in Raleigh NC and would love to speak with you regarding the possibility of implementing a battery recycling program at your campus as well as partnering with you to purchase the batteries that you collect. Please contact us at sierrametalsrecycling@yahoo.com. Thanks
On September 20, 2018, Jason Pearce wrote:
Lokesh Tripathi, do you pay 1500 USD per ton of lead acid auto batteries?
On August 31, 2018, Shaik Riyazur rahman wrote:
We r purchasing all types of Scrap batterys in Hyderabad My contact number is:.+91 90520 10000.+91 8309838948
On August 23, 2018, Gonzalo Megarejo wrote:
We have 120 tons for monts battery car used for sale...we are in Chile country. ... covir318@gmail.com
On August 20, 2018, General Trading US wrote:
Hey Guys, we are looking for tons of bad/old and unusable auto batteries to purchase at wholesale and if anyone/company has big quantities in USA and Canada please contact us @ generaltradingus@gmail.com and please provide your official company name, website, and phone number as well with detail of your products to see what you have and what are the models, quantities, wholesale price and etc..
On July 19, 2018, Samuel wrote:
Hey guys ,am new on this platform,i wanna sell lithuim iron lifepo4 battetries new and dead battery for a cheap price contact @ funnysamuel@gmail.com or via whatsapp +2347034573868
On July 3, 2018, MR Idowu wrote:
i am a supplier. you can get back to me on my email or whatsapp akoredesoneye@gmail.com or +2348172597402
On June 22, 2018, Mehrdad Dehghani wrote:
Dear Ms Cardano, Referring to your message dated April 8th -2018 at Battery University.com forum, We intend to start up a Battery collecting network across the country, from Laptops, Notebooks, Pads, Cellphone, Portable Powertools & toys using rechargeable batteries, and would appreciate it if you inform your more preferred type of batteries for your recycling plant, so that we can collect and store to reach 10-20 tons to ship to you in China. I would also appreciate it if you indicate an approximate price for your announced preferred batteries in above. I am on Skype, WhatsApp etc... on +98 912 348 6231 Thank you & Bst Rgds MD
On June 19, 2018, Mohit Agarwal wrote:
Hi I am interested in buying used lithium batteries. Suppliers can contact me from any part of the world. Thanks.
On June 6, 2018, MR Idowu wrote:
i have used cell phone batteries for sell. i am from nigeria. i have tested good one. i have the blue and the green result i have up to 135 tons now. please i only need serious buyer to contact me. my cell phone is +2348172597402 am on whatsapp and wechat too. please and please only serious buyer ok
On May 9, 2018, Muhammad asim wrote:
I am looking regular used or scrap dry battery supplier in USA my cell 516-728-7942 if you can provide auto batteries in bulk or container load every month
On May 2, 2018, David A wrote:
Anyone interested in buying used batteries from phones, laptops and other items from Uganda, please advise on kenninvest@gmail.com
On May 1, 2018, Riyas wrote:
Hi I wish to import scrap batteries to India if you have any idea about this please give me the information
On May 1, 2018, Abdul Akinpelu wrote:
I will like to have use battery recycling factory and where to get the machine
On April 24, 2018, Lokesh Tripathi wrote:
Dear Sir, How are you! Glad to know that you want to set up a plant related to recycling, I like to introduce myself as a Manufacturer of special purpose machinery related to recycling and setting up existing plant in more economical manner. Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market of $33 billion, lead acid (Car Battery) is the most common battery in use. As per the battery chemistry Lead Acid market value per ton is equal to $1500 which is highly profitable venture to start up also it remains the most suitable battery to recycle; 70% of its weight contains reusable lead. Now as per my understanding you want to recycle 10 tons of car battery per day right! We recommend 03 tons of Rotary Furnace with pollution control equipment keeping environment as a necessary aspect. Whole process will work like this: Stock of Used Car Battery -> to the battery cutting machine -> desulphurisation of acid from lead -> desulphurised lead sent to furnace -> ingot bullion casted -> sent to refining kettle furnace -> Refined Lead is stacked in Ingot Casting Conveyor. Our Innovative technology, Design, Precise workmanship, Prompt after sale service has edge to meet demands of today’s industry. The turnkey capabilities allow us to support our client with any types of job from relining Containers to major installations Should you however need any additional information or clarification in process of finalizing the above 0requirement. Please call us or write to us. Mean while thanking you & assuring you best of our services at all the times to come. We remain… Your prompt reply shall be highly appreciated. Please contact Me: Name : Lokesh Tripathi PH:0091- 9711141615 Location : India , Delhi, (NCR) Email: info@indotherm.co.in
On April 22, 2018, Ghazi wrote:
Hi all, i want to open plant recycling of batteries in Saudi Arabia i need your help plz as i dont have any information abouy the best company to buy the equipment
On April 12, 2018, Imran Khan wrote:
Hello Suzan, Please watsup me@ +918123561118 for the information related to recycling. Thanks Imran
On April 11, 2018, Fatima Susana Martinez Lopez wrote:
To whom this might concern, Hello, my name is Fatima Susana Martinez Lopez. I am currently an honors student at Wake Technical Community College in the state of North Carolina. I have been working on a research project about batteries and I noticed that many people that attend my college campus do not know how to properly dispose of their old batteries. Currently, there is not a specific battery recycling program. While working on my research project my honors advisor and I were discussing how to initiate a battery recycling program on our campus. So, I came across your website and I am impressed at how well organized you are about recycling batteries. By any chance, could you give us some advice from your experience on how to implement a Battery recycling program like yours on my college campus? We are mainly interested in the logistics of how to properly collect the used batteries but any advice would be greatly appreciated. Sincerely, Fatima Susana Martinez Lopez
On April 9, 2018, Cardano Li wrote:
This is Cardano.Our company wants to buy dispose/waste/scrap lithium battery as much as possbile. Our company capacity is 10,000 tons/month, so we try to collect worldwide. For price, it depends on the kind of waste lithium battery, when we have picture, we can estimate the price. From you, if you collect enough 20 tons for one container, we can buy immediately and export to China.We now need to purchase recycled products: I: Finished products: scrapped laptop battery, scrapped battery, scrapped cell phone battery, scrapped electric vehicle battery II: Material:Cathode film scrap (lithium cobalt),Cathode film scrap (Ternary Lithium battery),Battery core scrap (Lithium cobalt without liquid) ,Battery core scrap (Ternary Lithium battery without liquid),Battery liquid core scrap (Lithium Cobalt),Battery liquid core scrap (Ternary Lithium battery) ,Cathode powder scrap,Cathode slurry scrap (Lithium Cobalt),Anode film scrap,Cathode slurry scrap (Ternary Lithium battery)。 I send to you my skype: cardano.lee, please accept and then we can discuss easier. our factory 10 years focusing on reproceeding waste Li-ion battery with environment friendly way and advanced high technical method.Is t possible to take chance for cooperating with your company based on mutrual benefits? Hope to hear from you soon with my sincere appreication. Thank you and Best regards Ms Cardano Li (wechat / what'App : +86 18503066565 ) Global Purchasing Director Skype:cardano.lee Email:purchaser@recycling.org.cn
On March 31, 2018, Kashif Tai wrote:
Hi All, I am looking for Lead Powder /Paste in big quantity every month. If anybody can offer me, please let me know soon. Regards Kashif Marium.ent@hotmail.com 00923219210739
On March 21, 2018, Open Technology Park wrote:
My Dear Friends, to match used batteries buy/sell offers we need on-line transaction exchange system, known from solar panels market. To make things short, just make your offer real, give your buy/sell price, give your geolocation to let us calculate pick-up or delivery costs / courier + your price to make trade offer profitable for both parties. Please be aware, email by gmail is not supporting business talks, since your reply can always be sent to trash or spam box and it takes a lot of time to track thread. Linkedin or Twitter are real-time chat services, so you can talk and get immediate response and make business on-line. If you know how can I get and buy 100 used Li car batteries per month or a stock of 1,000 in Europe, please let me know, since I don't love the idea every used Li car battery should be recycled. I have already given second life to hundreds of Li, Pb used batteries and it makes sense. This month I start tests with garage production of gel batteries since sulphur acid new or used car batteries are of limited use off-grid renewable energy systems due to risk of acid leakage Let me know if you can use Twitter best regards, Open Technology Park Open Fabrication Lab Darius Jack jack.investigator@yandex.com Twitter: jack.investigator@yandex.com Twitter support personal messages and notifications and images can be easily attached, as well as web links
On March 19, 2018, Trang wrote:
Dear Simone Can you share your stock information? We would like to buy a big volume of lithium battery with comparetitive price Best regard email: dianaross.smith@gmail.com
On March 17, 2018, Trang wrote:
Dear Dinesh Could you contact to me in email My company has plant to set up factory in other countries once these countries has enough capacity of lithium battery scrap to run (at least 600 tons month). Could you tell me about the potential there skype cupi2013
On March 17, 2018, Hakim wrote:
Hello plz email me if you you want to buy recyclable car batteries hakeem_esdeen@hotmail.com
On March 9, 2018, darius wrote:
Hi Simone, since I don't get reply from you and gmail.com is no more reliable today, not supporting re: re: re: Please email me at jack.investigator@yandex.com Open Technology Park This is my email sent to you, not replied yet. -- Thank you Simone for your kind reply. First image: 90Ah Li cells by Headway (f. Winston), installed some years by a company from Italy, converting Fiat Doblo to all electric. I am interested. The problem is these Li cells simply swell ( pillow effect), not fit for EV since can broke apart any closed apartment for batteries ( 74 in series). I have a number of them under my table, completely discharged ( nominal voltage is 3.2V , today 0.2V) Images 2 and 4 e-bike packs, really inrterested in, since I build intelligent Li-Ion spot welders and use old Li-Ion cells for tests. Image 3 Li-Po cells and packs, swell badly, should be recycled as soon as possible since can get a fire at random. I recentl;y purchased Li-Po power bank (new), which burnt out at the shop, still in original box, so I was not aware of. Image 5 - old Ni-H cells from e- tools, old technology, no use , I recycle them. Please let me what number of 90Ah cells by Winston and what number of e-bike battery packs ( BMS, balancer module removed) can be collected and what are your terms. I am looking for modern battery packs for Tesla, Toyota Hybrid and other EVs best regards, Darius
On March 6, 2018, darius wrote:
Hi Simone, interested in your li-ion batteries from Ev and e-bikes. Let me know your geolocation and attach some images of your stock darius Open Technology Park manta103g@gmail.com
On March 6, 2018, Simone wrote:
Hello, we have lot of used li-ion batteries from Ev and e- bikes, most of them still have capacity. Anyone interested into buy them?
On February 25, 2018, mr emeka wrote:
Hello, I’m a Business man. Beside my study I run a big business on lead battery recycling. I collect scrape battery from many districs . I just buy scrape batteries which are used in bus, truck, car, auto, motor bike, ips, solar, cng, telecommunications tower, touch light batteries and so on. From recycling this I come out pure lead and sell to my nearby company. But at now I want to export lead to foreign countries. If any one want to buy lead from me please contact with me via email. also sell lithiums batteris My email :- emekabattries@gmail.com
On February 25, 2018, mr john kojo wrote:
Hello, I’m from ghana. I’m a business mant. Beside my study I run a small business on lead battery recycling. I collect scrape battery from many districs . I just buy scrape batteries which are used in bus, truck, car, auto, motor bike, ips, solar, cng, telecommunications tower, touch light batteries and so on. From recycling this I come out pure lead and sell to my nearby company. But at now I want to export lead to foreign countries. If any one want to buy lead from me please contact with me via email. My email :- mdsharifulislam.msis@gmail.com
On February 25, 2018, mr john kojo wrote:
i have lithium battrties and acid battries used for sell in tons
On February 24, 2018, fiona wrote:
looking for lead acid battery from world . if you know where to get,how to get ,who can supply, pls let me know here best regards fiona wechat:+0086-15356118280 oopscolor @ 163 . com
On February 22, 2018, mr john kojo wrote:
i sell lithium's batteries in tons if you have interest of buying from me. you can contact me on my email or whatspp. email: johnkojomarketing@gmail.com. whatsapp number is +233552263100
On February 19, 2018, viswanadh wrote:
Hi,i'm planning to start battery scrap dealer in andhra pradesh india. my question is what are the license required to start this... Please help me.
On February 2, 2018, Andy Jung wrote:
Dear All We are recovering valuable metals from LIB in south Korea. I am looking for LCO or/and NCM powder from the used LIB. Please contact me if you can supply such powder materials. Thank you. Andy Jung chemtex.jung@gmail.com
On January 23, 2018, darius wrote:
Hello Dinesh, I am not sure about profitability of Li-Ion battery recycling plant, since you need to apply for public funding, subsidy first. I am interested to buy largest Li-Po Li-Ion batteries by size, weight and current (Ah) and offer regeneration, preselection technology since it makes sense to refurbish and give second life to such expensive electric hybrid car or bus Li-Ion batteries. Just purchased 85 90Ah Li-Ion from electric car and started regeneration process. Many may claim it doesn't make sense. Exactly, but I already succeeded to regenerate Pb car batteries, gel batteries and what comes next are exactly Li-Ion heavy current, amperage batteries since the price of new ones is great challenge. I am going to buy Toyota Prius electric and hybrid battery packs for regeneration. Since Li-Po, Li-Ion battery transportation restrictions apply, I am not going to import large quentities of Li-Ion large current batteries from one continent to another to meet all safety regulations and cut the costs. I would like to establish a network of Li-Lion batteries world-wide and deliver technology solutions, professional chargers and general guidance. 10 years ago I regenerated large quantities of Li-Po Li-Ion cell phone batteries with great success due to limited availability at local markets. Let me know your opinion and your interest Darius Jack Open Technology Park manta103g@gmail.com
On January 22, 2018, dinesh wrote:
Hi, I m looking to set up a Lithium ion base battery recycling plant with most efficient way to extract lithium and other metal. kindly guide me that which companies are offering help to set up in India
On January 10, 2018, darius wrote:
Hi David, Hi Allan, I have already emailed you you have some options open. In Europe VRLA Pb batteries are collected for free by recycling plant or its agents, or you can negotiate a price per kg, as a source of Pb metal. Other option is to diagnose every battery and use fast charger to get some back to life and sell as used VRLA batteries at half price. If you know what are the sources of used VRLA ( large or small UPS system, security system, medical equipment , personal use) I can tell you more. Just list me Amperage (Ah), Voltage (V), size, type, manufacture year by manufacturer. Since East Africa lives close to China, local market prices of new or refurbished VRLA batteries may be much lower vs. Europe. I am interested to import your VRLA 150Ah batteries to Europe for some refurbishing-recycling procedure Darius Open Technology Park manta103g@gmail.com BTW , just attach some images
On January 9, 2018, David A wrote:
Dear Sir/Madam, I have 1,000 pcs of VRLA Batteries (12v, 150ah) for Recycling or Regeneration in Rwanda(EA) and seeking ideas & partners to do this in the shortest time possible. Similar opportunities apply for othe East African countries (Uganda,Ke,TZ, Juba) Please advise on kenninvest@gmail.com
On January 5, 2018, Trang wrote:
Dear Sir/Madam NEED TO BUY A BIG QUANTITY OF UNUSED LITHIUM BATTERY FROM JAPAN/INDIA. My name is Trang. I am a marketing manager of ANHUA TAISEN RECYCLING COMPANY. .Our business is recycling dispose lithium battery (18650 batteries) in our factory in China including: cell phone battery, laptop battery, electronic car, industrial railway battery, aviation battery…. we need to buy/ import a huge of dispose/unused lithium battery in Japan/India with whatever status of battery. We are looking for the source of unused lithium battery to buy, if you have or you know some kinds of unused lithium Battery Company/ manufactures/seller in Japan/India who wants to sell, please introduce to me. Look forward to getting your news. Best regard My email: trang-marketing@tai-sen.cn
On January 2, 2018, Maureen Onwuka wrote:
SUPPLYING USED BATTERIES Hello, i recently got into the supply of used inverta battery when i was contacted to supply a certain quantity here in Nigeria, West Africa by an Organization that was exporting same to Europe in 2016. I have been doing research on the market for battery recycling and i know the business to be lucrative though tedious. Now am interested in this business but mostly in the supply of the Starter battery (Cars, Automobile), Traction (Electric Car) or Stationary battery (Power Supply). Please anyone that is interested to get them from Nigeria should contact me. Nigeria is a veritable ground for this business due to the high usage of batteries because of power shortages and the need for alternative sources as well as the population of car users which is quite high. Kindly respond. Regards, Maureen Onwuka nikky2002ng@gmail.com
On December 31, 2017, Junaid wrote:
I am intrestes in this business scrap and battery recycle. I am from india if anybody intersted Contact me +919015367919.... syedmashkoor4@gmail.com
On December 25, 2017, Saeed Ur Rehman wrote:
Hi All, I am Saeed from Jeddah Saudi Arab and I have a Lead refining factory and I want to start my business in Pakistan anyone who can help me in this regards can contact me as I have some queries about this factory also about the remaining material after recycling the lead from batteries I need any research center any were in the world you can easily contact me on my Whatsapp, IMO, FB NO 00966580002834,00923129890459 or Saeedlucky@icloud.com
On December 18, 2017, Walter Esteves Incio wrote:
Excelente informacion, soy experto en reciclaje de baterias, experiencia maa de 30 años Plomo bulion, refinado al 99.99 %, plastico, soluciones acidas etc mi correo es: esteveswalter1@gmail.com
On December 18, 2017, Walter Esteves Incio wrote:
Experto en Reciclaje de baterias plomo acido, PP plastico de cajas, soluciones acidas, Plomo Bullion, Plomo refinado 99.99 %, plantasde oxido de plomo. Diseño - Fabricacion en cualquier escenario, baterias industriales, etc., mi ciorreo electronico es: esteveswalter1@gmail.com Tesis de grado en topicos de reciclaje
On November 6, 2017, samer wrote:
hey dear ; we have monthly 300 mobile phone batteries we love to know prices about it and if u have free shipping..... thank you, waiting your request.
On November 2, 2017, haiytham wrote:
interested pl. contact me
On November 1, 2017, MOHD RASHID wrote:
Require in bulk quantity spent mobile Lithium ion batteries for Recycling. Please contact; 91-7550633477 e-mail; arkrashid20@gmail.com
On October 13, 2017, abdul moiz wrote:
we have large number of silver oxide button cells .we are looking for some buyers for these kind of batteries . kindly contact on 00971558789898.
On September 23, 2017, Mohammed wrote:
I am looking to start recycle of scarp batteries I would like to know more about the field of recycling and demand in the market. My contact number mentioned below Thanks Mohammed 00917010317274
On September 18, 2017, Kristina Malgina wrote:
We are a trading company in Hong Kong. Currently one of my clients is looking to buy a large amount of used lead-acid batteries (500-5,000 tons per month) to be shipped to our port. We do not have a preference on the exporting country, as long as the supplier is reliable and cost-effective. However, I do not have experience with lead-acid batteries specifically and am struggling to find suitable candidates for such exports. If you are an individual who has information regarding where I can find such exporters, please do reach out - any information would be helpful. If you are company that is able to fulfill such requirements or are looking for a buyer, please do get in contact with me via email- I would be very happy to hear from you. Thanks in advance! kristina.malgin@gmail.com
On August 15, 2017, Optimum Battery wrote:
We are a Saskatoon based business that sells used/refurbished automotive batteries and provides battery collection/drop-off services to the surrounding area. We try to Reduce, Reuse, and Recycle - therefore, each battery we collect is tested, and if possible refurbished for resale before it is eventually recycled. If you are an individual or business in need of a solution to your constant scrap battery accumulation, please don't hesitate to contact us! Check out our website at www.optimumbattery.ca
On August 6, 2017, Sulaiman Meghjani wrote:
We are Toronto and UK - Hounslow based looking for opportunity into battery recycling. We can be your reliable partners in Collection, managing stocks etc at these locations. If any body is interested in sharing revenues, please contact us info at grinva . com sulaimanmeghjani at yahoo . com
On July 15, 2017, RAJAT ANAND wrote:
Hi, We at Mettherm, provide complete turnkey solution for Battery Recycling for extraction of this lead in usable form. We provide Battery Recycling Plants, Lead Ore Smelting Plants, Lead Refining Plants, Battery Breaking and segregation plant and consultancy till trial production. You can visit our website mettherm.com for more details and can also request for a quote depending on the capacity of the plant required. We are based in Faridabad, New Delhi NCR, Haryana Thank you, Rajat Anand
On July 7, 2017, darius wrote:
Hi, could you kindly explain, why emailed submissions from this page get delivered as unformatted ASCII text email, making hard to read them ? Ok, I know an old End Of Line / New Line formatting problem in Linux vs. MS Windows problem, already solved 20 years ago. Could you upgrade serveer settings to deliver formatted submissions via e-mail ? Already recycled 10,000+ Li-Ion used batteries, giving them second life. thank you darius
On July 6, 2017, american manganese wrote:
AMERICAN MANGANESE INC. REPORTS WORKING RECHARGEABLE BATTERIES PRODUCED FROM RECYCLED NMC CATHODE MATERIALS Kemetco Research Inc. has successfully produced lithium:nickel:manganese:cobalt (Li:Ni:Mn:Co) (NMC) cathode material and working coin cell rechargeable NMC batteries using recycled lithium, nickel, manganese and cobalt from American Manganese Inc.'s patent-pending lithium-ion battery cathode material recycling process. Preliminary battery cycling test of the NMC battery has demonstrated that it reached the targeted battery capacity, which further proves American Manganese's patent-pending battery recycling process can recycle and refabricate the NMC material to make new NMC batteries. "Based on these preliminary results," said Norm Chow, president of Kemetco, "it can be speculated that the American Manganese upcycling technology represents the world's first NMC battery produced from AMI'S closed loop recycling process." "These results continue to validate the AMI process," said Larry Reaugh. "With this phase of test work, we've taken very complex lithium-ion battery cathode material from the recovered components through the reconstitution of the NMC cathode materials to produce working chargeable cells." Battery fabrication and assembly Recycled NMC was generated by precipitating the metal components from a leached solution of commercially available feedstock. XRD (X-ray diffraction) of the reconstituted NMC material has characterized the material as having a perfect ratio of Li:Ni:Mn:Co -- 1.06:0.33:0.33:0.33 -- a 100-per-cent match to the commercial battery grade of NMC. This cathode material mixture was subsequently coated onto aluminum foil and dried for two hours at 120 C in a vacuum oven to form the lithium-ion battery cathode. The button cell batteries were assembled as follows: top cell case, cathode, separator, anode, spacer, ring-shaped spring and bottom cell case. The anode was made from purchased graphite. The ring-shaped spring was placed between the negative casing and the spacer to ensure adequate pressure was applied to the cell components. Both the spring and the spacer are made from stainless steel. A thin layer of polyolefin was used as the separator. About American Manganese Inc. American Manganese is a diversified specialty and critical metal company focused on capitalizing on its patented intellectual property through low-cost production or recovery of electrolytic manganese products throughout the world, and recycling of spent electric vehicle lithium-ion rechargeable batteries. Interest in the company's patented process has adjusted the focus of American Manganese toward the examination of applying its patented technology for other purposes and materials. American Manganese aims to capitalize on its patented technology and proprietary know-how to become and industry leader in the recycling of spent electric vehicle lithium-ion batteries having cathode chemistries such as: lithium-cobalt, lithium-cobalt-nickel-manganese and lithium-manganese (Please see the company's Jan. 19, 2017, press release for further details).
On July 4, 2017, american manganese wrote:
http://americanmanganeseinc.com/ American Manganese Inc. is a Critical Metal Company Focusing on Recycling Lithium Ion Electric Vehicle Batteries. there you go!
On July 4, 2017, Sridhar wrote:
Hi all This is sridhar from Chennai Am very much interested in this business but I don't have any idea about this. Am looking for the investor to start this business. I can arrange land and all licence to start this business. If any one interested to expand your business at Chennai please contact me at Sridhar 919543342667
On June 16, 2017, Md Shariful Islam wrote:
Hello, I'm from Khulna,Bangladesh. I'm a student. Beside my study I run a small business on lead battery recycling. I collect scrape battery from many districs . I just buy scrape batteries which are used in bus, truck, car, auto, motor bike, ips, solar, cng, telecommunications tower, touch light batteries and so on. From recycling this I come out pure lead and sell to my nearby company. But at now I want to export lead to foreign countries. If any one want to buy lead from me please contact with me via email. My email :- mdsharifulislam.msis@gmail.com
On June 14, 2017, Imran Khan wrote:
Hello, Nazmul hasan. Please contact me my factory is for sale in India, also share your contact Contact or Watsup 919341836119
On June 13, 2017, Nazmul Hasan wrote:
Hello This is Nazmul Hasan from Bangladesh.I need a small lead Battery recycling plant 10ton daily waste scrap ,dross My finished goods will b hard lead/raw lead Low investment XENCELL Battery Ranabola,Taslima plaza Turag-Dhaka-1230
On May 30, 2017, yerry easy wrote:
Write us today on yerryeasy@hotmail.com, we can be your agent/representative. Also we can help you with recycling services.
On May 20, 2017, Naveed Shaikh wrote:
Dear Mr. Subrata Pal, Please contact us @ 91-9987077382
On May 19, 2017, Subrata pal wrote:
I want to start battery recycling business in India , in India state of Tripura . Essential machinery for this purpose...
On April 19, 2017, Mansoor wrote:
I want to start battery/battery recycle business in Afghanistan, the opportunity is very good for such business in here, the demand is very high here, All I want is to have an expert to guide me trough the start of business or guide me to have essential machinery for this purpose. Anyone who want to help me please reach me with email below; mansooraziz16@gmail.com
On March 28, 2017, Sohan wrote:
Hello We are lead acid batteries manufacturer and recycler in India (Rajasthan). We have been in this business from last 10 years. If any one like to start this business in India we can help in all feel free to contact. We would also like to establish lead acid recycling plant outside India as well. Thanks sohanchouhan3@gmail.com +919784289007 (WhatsApp) skype:sohan2479
On March 3, 2017, anita wrote:
Hello have you been search for scrap metals , you have found the right place were you can get your urgent scrap metal. search no further, We sells Scrap metal recycling and scrap metal yard, We also Sell recycle metals of all types, shapes and sizes. Our metal scrap yard is equipped to handle small loads of household metal scrap and large loads of commercial scrap metal salvage. We sell metals at the lowest prices and have a reputation in the Valley of the Sun as being fair, honest and professional.EMAIL: clintonmathewscrapmetalcompany@gmail.com whatsapp or call +2347059186258
On February 9, 2017, Lokesh Tripathi wrote:
Dear Sir, How are you! Glad to know that you want to set up a plant related to recycling, I like to introduce myself as a Manufacturer of special purpose machinery related to recycling and setting up existing plant in more economical manner. Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market of $33 billion, lead acid (Car Battery) is the most common battery in use. As per the battery chemistry Lead Acid market value per ton is equal to $1500 which is highly profitable venture to start up also it remains the most suitable battery to recycle; 70% of its weight contains reusable lead. Now as per my understanding you want to recycle 10 tons of car battery per day right! We recommend 03 tons of Rotary Furnace with pollution control equipment keeping environment as a necessary aspect. Whole process will work like this: Stock of Used Car Battery -> to the battery cutting machine -> desulphurisation of acid from lead -> desulphurised lead sent to furnace -> ingot bullion casted -> sent to refining kettle furnace -> Refined Lead is stacked in Ingot Casting Conveyor. Our Innovative technology, Design, Precise workmanship, Prompt after sale service has edge to meet demands of today’s industry. The turnkey capabilities allow us to support our client with any types of job from relining Containers to major installations Should you however need any additional information or clarification in process of finalizing the above 0requirement. Please call us or write to us. Mean while thanking you & assuring you best of our services at all the times to come. We remain… Your prompt reply shall be highly appreciated. Please contact Me: Name : Lokesh Tripathi PH:0091- 9711141615 Location : India , Delhi, (NCR) Email: info@indotherm.co.in
On February 7, 2017, Abraham wrote:
I am impressed with this business as it offers great opportunity. I visited a Battery Recycling plant some months ago and I love to start up same with aid of foreign partners. Anyone with detailed plan of this business, should reach me via the email. holuafolayan@gmail.com
On January 31, 2017, pawandeep singh wrote:
hi Beth, kindly share your contact details. we can help you. thanks CrossBar wrote: Hi, Im looking for a company that would recycle/dispose large quantities of Lithium Polymer batteries, coming from e-cigs for 70-80K month. Could you point me in the right direction? THANK YOU Beth Barton
On January 23, 2017, Dr. Venu Katta wrote:
Hello Everyone, Firstly, I would like to introduce myself, I am Dr. Venu Katta, x Director & VP for Exide Technologies Canada. I always had a dream to start a Lead Acid Battery Manufacturing Plant in India. I lived here in Canada for past 20 Years, recently I moved to India to start the Lead Acid Battery Manufacturing Plant in south part of India. I then procured Land and Constructed the Unit with North American Standards. I have all the Licenses which includes Red Category Pollution License and Small Scale Industry License and all other Industrial Licenses in place issued by the Pondicherry Government. Due to unforeseen reason, i have to move back to Canada again. If anyone is interested to take over the project along with the land and building with HT approved electricity in place. I am ready to sell the property and or if someone is interested to lease the property i am willing to give away the Mobile entire established project. Please contact me for further details either via phone or email. My contact information is Mobile Number 001-905-531-2551 and email id: v.katta@hotmail.com. I thank you all for your kind cooperation and appreciate your support and help in advance! With Best Regards, Dr. Venu Katta
On January 17, 2017, Debaraj Mishra wrote:
Hi My South Korean company would like to start lithium ion battery recycling unit in India soon. We would like to contact as many as suppliers who can supply waste LIB batteries. Is there anybody who would supply such materials to us regularly? Thanks. mail me debraj.mishra@gmail.com
On January 9, 2017, Tarun wrote:
Hi, I am in battery field for around 12 years. I have battery business (start-up) in North India. I have well established market (dealers/distributors). Is any person interested to invest in my business? Also, I am looking for manufacturers, who can provide me automotive/inverter batteries. Thanks
On December 28, 2016, Malyasee wrote:
I am an expert in setting ups a" Lead Acid Battery Recycling Plant" with less capital cost,any one interested do let me know, Thanks
On December 14, 2016, CrossBar wrote:
Hi, Im looking for a company that would recycle/dispose large quantities of Lithium Polymer batteries, coming from e-cigs for 70-80K month. Could you point me in the right direction? THANK YOU Beth Barton
On December 13, 2016, Balaji wrote:
Hi all, We are leading suppliers of lead acid battery scraps in Tamil Nadu, India established in the year 1997. We can supply minimum of 150MT per month. Kindly contact us by phone +91-96262-52520 or email to balaji@electroindia.net We are interested to buy battery scraps from other countries. Necessary import certificates are available. Kindly contact us to discuss further. Regards, Balaji +91-96262-52520 balaji@electroindia.net
On December 11, 2016, paul wrote:
have large regular amount of phone batteries for recycling serious inquiries please
On December 2, 2016, farsad wrote:
I look forward to hearing from you. Email :infoelcatek@gmail.com
On December 2, 2016, farsad wrote:
We supply lead acid scrap. Any interested buyer should please email to get details.
On November 16, 2016, Wald wrote:
Dear Sirs. I have a great amount of scrap batteries monthly to recycle in Paraguay South America. If there is any company with logistics to pick up the batteries are very welcome. Please send a list of price for my email with the prices that you pay for each type of battery by Ton. Thanks..Wald..Whatsapp +595983132181
On November 16, 2016, okoso wrote:
I am based in Mongolia and want to setup a Lead Acid Battery Recycling Business. Any information will be greatly appreciated. Thank you okoso13@yahoo.com
On November 6, 2016, Sandeep wrote:
I want start smelting battery lead scrap in electric machine what's the process and how much time 50 kg battery lead scrap melting process and 50 kg battery scrap after melt not plastic only lead scrap how much quantity or kg after smelt I receive solid lead in 50 kg
On November 5, 2016, Christian wrote:
Hello I am WEEE recycler based in Lagos state of Nigeria. i have large lithium stock of scrap batteries and have the capacity to increase depending on Mou with a buyer. $1.12/lbs I seek buyers. kindly email cademicsgroup@gmail.com Christian +2347012733347
On October 30, 2016, Fahad wrote:
I want to setup a modern Lead Acid Battery Recycling plant in Pakistan , anybody can enlighten me about availability of Lead Acid battery scrap and feasibility and survival of this industry Thankyou waiting For reply Email sales@faithmetal.com.pk
On October 27, 2016, Imran khan wrote:
Hello, I saw many of them looking for used battery recycling plant . Please contact Aleem khan +919341836119 or +918123561118 . We are planning to sale our battery recycling plant located in India with all pollution control board of India certificate plant full loaded running plant with all machineries and equipments along with land .all certificates are updated and valid.serious person who is looking for battery recycling plant buyer can contact us. Thanks, Imran khan 8123561118 Sent from my iPhone
On October 26, 2016, Haider wrote:
How can one obtain a license to produce green lead
On October 26, 2016, Lubna Hanif wrote:
Looking for used car lead battery recycling plant. Any information will be greatly appreciated. lubnahanif583@gmail.com
On October 25, 2016, JS Kim wrote:
I am looking for companies who requires 'battery recycling' Our company(south korea) is very qualified and well experienced in field. We already doing buisness with recycling batteries in china, India, Turkey and South Africa. We can do all kinds of batteries in any term. Pls contact me If you interested; Jiseonkim0807@gmail.com +91 9618098812 ( india ) +82 10 3906 6445 (Korea )
On October 23, 2016, Lubna Hanif wrote:
I am based in California USA and I am desperately looking for Car battery recycling plant. If anybody can help me with information. I will be really grateful.
On September 28, 2016, Rahul wrote:
hello Can we get in anybody india scrap seller /buyer contact-8103095763
On September 23, 2016, leila wrote:
Hello I want to set up Ni Cd waste batteries recycling plant.please can anybody help me with information especially Pyrometallurgical method to recycling battery. Thanks Email:z.khamooshi@gmail.com
On September 21, 2016, leila wrote:
Hello Iam studying master chemistry engineering.my project is Recycling Of Valuable Metals From Nickel Cadmium Waste Batteries.I will do my tests other weeks but I have some problem about process if you can help me please guide me.thanks Email:z.khamooshi@gmail.com
On September 10, 2016, Amol Jadhav,Pune wrote:
We have designed a technology where no need to replace the old battery.Its environment eco friendly cost saving project to all Battery users.Pls revert if interested on +917066667883.We can start business any where in India.
On August 31, 2016, Leonard Dugan wrote:
Hello, Looking for a company in the Dallas / Ft Worth area that buys li-ion, NiCad, NiMH, batteries. I have batteries and cells from home use, medical equipment, laptops, drills, etc. please email me or post the information here. I have around 500 pounds total to sell. Thanks Leonard
On August 29, 2016, Raju Penumatcha wrote:
Hello Pawan Mundra, we can propose a business model for Lead Acid Battery re-generation, with capital requirement far below that of re-cycling. re-generation allows, pollution free, profitable Lead Acid Battery business. let us know your interest. raju_pvr2006@yahoo.com Raju
On August 29, 2016, pawan mundra wrote:
I want to set up Lead Acid Battery Recycling Plant.
On August 26, 2016, muhammad iqbal wrote:
''consumption ,preparation ,import and recycling of batteries in Pakistan.''
On August 14, 2016, Gibson John wrote:
Hello everyone I m looking for a serious partner I can sign a contract with because I have about 30 tons of drean lead acid scrap battery in stock already and I can export to any country only serious buyers should contact me please and I will show you our goods that is already in stock by picture through email thanks Email giggslan80@Yahoo.com or giggslan80@Gmail.com Or u can reach me on phone +23408181039941 . Best regards Gibson John
On August 13, 2016, Naveed Shaikh wrote:
Dear, Anybody with availability of Lead Acid Battery Scrap please let us know by email. To introduce ourselves, we are a 30 year Old Company based in Mumbai, India in the field of Lead Oxides, Lead Battery Recycling & Battery Manufacturing .We are manufacturers of these equipment and undertake such Projects on Turnkey basis. Consultancy is also a part of our service. Our Company is a team of Well Experienced technocrats who have experience of more than 35 years Individually. We have executed projects in Indian Sub Continent, Middle East, Africa, Far East and Russia. We have 70 projects to our credit. sales@acsleadtech.com +91-9987077382
On August 11, 2016, jas wrote:
Hi! there, I want to setup a lead acid battery recycling plant in India for a capacity of 10MT / daily. I want start with small unit first. please can anybody help me with building up of plant. Preferably I like to setup this in Uttar Pradesh, India
On August 8, 2016, Raju Penumatcha wrote:
Hello A K, we offer technology and training support, for Re-generation of Lead Acid Battery. -- curative re-generation would allow extending the life of a used ( end-of-life) lead acid battery by an additional 100% -- preventive maintenance would allow in-use lead acid battery by an additional 100 to 150%, and also reduce the energy used for charging, over the use of the battery life. we are interested to offer the idustrially proven technology and training is available. best e-mail: raju_pvr2006@yahoo.com
On August 6, 2016, A K wrote:
Hi All, I want to setup a modern Lead Acid Battery Recycling plant in Nigeria, anybody can enlighten me about availability of Lead Acid battery scrap and feasibility and survival of this industry in terms of Nigerian economy and present situations. Proposed capacity is 100MT/day.
On July 30, 2016, Raju Penumatcha wrote:
Hello Sasi Gopalan, please contact us at the e-mail address. we have a business proposal for re-generation of Lead Acid Battery. best e-mail: raju_pvr2006@yahoo.com
On July 28, 2016, Sasi Gopalan wrote:
I am interested in starting a battery recycling unit/new unit. Can somebody help me with technical details, where to buy machinery etc.
On July 25, 2016, Khalid Shamsher wrote:
I am interested in setting up a lead-acid battery recycling plant in Pakistan. Finances are arranged already. Need proposals from experts for supply of whole set-up. The objective is to use recovered sulfuric acid for agriculture usage and re-use of lead ingots for battery manufacture. regards, Khalid 0092-300-3308918
On July 20, 2016, Open Technology Park wrote:
Hello Swarock, interested in your offer. Please email me manta103g@gmail.com Darius OpenTechnology Park Swarock wrote: We have a huge stock of LIB batteries from electric & hybrid vehicles. Looking for service partners who can collect, transport(with proper packing as per local regulations) and recycle the batteries. The regions we are looking at are as per priority are: 1. West Europe (Germany, fra, ita, spain, scandinavia, UK) 2. East Europe(Russia & neighbors) 3. China & neighbors 4. USA & Brazil Licenced and certified recycling service partners only. Mail me at edspcommerce@gmai.com for further details.
On July 19, 2016, Raju Penumatcha wrote:
Hello Leeban, please contact me at the e-mail address. we have a business proposal for you. raju_pvr2006@yahoo.com best
On July 19, 2016, Leeban wrote:
We have a scrap lead battery more than 2000 ton for sale in Ethiopia we can export to any country
On July 19, 2016, Chigozie Azunna Ekwuluo wrote:
I the above name and email address, leaved in Nigeria, I have 200 pieces of drained batteries for sell how will I do? In case you're interested simply reach me through my email or my phone no. 08171902879.
On July 18, 2016, Swarock wrote:
We have a huge stock of LIB batteries from electric & hybrid vehicles. Looking for service partners who can collect, transport(with proper packing as per local regulations) and recycle the batteries. The regions we are looking at are as per priority are: 1. West Europe (Germany, fra, ita, spain, scandinavia, UK) 2. East Europe(Russia & neighbors) 3. China & neighbors 4. USA & Brazil Licenced and certified recycling service partners only. Mail me at edspcommerce@gmai.com for further details.
On July 9, 2016, Mohd Rashid wrote:
We want to purchase lithium ion battery scrape in tons regularly on cash parties who can supply the material on competitive price can contact E-mail;arkrashid20@gmail.com Mob;9555502324 8802784136
On June 30, 2016, kishan jaiswal wrote:
We have in Kolkata, West Bengal some lithium based batteries to dispose off. Is anyone interested to purchase can mail us to kishan_jaiswal1@yahoo.com immediately.
On June 17, 2016, Raju Penumatcha wrote:
We are looking for those interested in re-generation of Lead Acid batteries used as 1) starter batteries ( cars, automotive) 2) traction batteries ( electric vehicles - fork lifts etc.,) 3) stationary batteries ( power supply ) the technology allows re-generation of upto 90 % capacity, and extend the battery life. re-generation can address : -- Environmentally friendly process -- reduce, re use and re generate those interested may please contact us for business opportunities. raju_pvr2006@yahoo.com Toronto, Canada
On June 17, 2016, ron pratt wrote:
take a look at Aqua Metals. 20% owned by Interstate Batteries. The Secondary Lead Recycling alternative to smelting http://www.aquametals.com/#about
On June 9, 2016, Open Technology Park wrote:
goodness, Battery recycling business is really hard business. In EU, US, Canada, Japan and most developing countries you need to be licenced and certified recycling facility to start with recycling. To recycle batteries you need to develop logistics and build network of battery collection points. In some countries, used batteries transported in quantities are subject to Environment Protection, Hazardous Materials handling restrictions. You need need to read carefully your local legislation if you are free to transport 1t of used batteries from City A to your location. If your stock of used batteries is large and new deliveries pending you can start with selection, separation and discharging in case of Li-Ion, Li-Po batteries. It's still too early to buy technology, chemistry, machinery, equipment, to build recycling facility from the scratch since in EU countries, electric and electronic waste recycling facility collects batteries by itself or gets them delivered as a waste to be disposed of. So In theory your stock of faulty batteries can grow without any investment. Buying new Pb car battery you pay extra recycling fee, about $10, so drivers expect to get recycling fee back on disposal of faulty Pb car battery. To learn more just email me manta103g@gmail.com Open Technology Park
On June 8, 2016, goodness wrote:
Hi Guys, i am very interested in this battery recycling business. Please if there is any information / Knowledge that can make it a success, kindly lay it out. i am very interested.
On May 17, 2016, Ranthi Dias wrote:
Please let me know if anyone using cleaning chemicals in the battery recycling industry. the cleaning chemical and the application?
On May 3, 2016, Leeban wrote:
Im from Ethiopia and i have more than 30p ton of battery to export and looking for buyers contact me my email address nebilq@gmail.com
On May 2, 2016, Shaikh waqar wrote:
Sir if i want to buy lithium ion cell scrap or laptop battery scrap what will be the procedure please contact or mail me on my id
On May 1, 2016, Aleems wrote:
Send u r mail id & contact number
On April 30, 2016, Najiib wrote:
I very happy to this jop, it's important to us, I am busines man, I have large country without recycling agency. So l want to help our county environment. And I am ready to this program.
On April 29, 2016, Natanael Moreno wrote:
I am looking for a company or several companies that can provide me at least 200 metric tons per month of lead-acid batteries. To import them to México. I want to get in touch with companies in the USA. Hope you can help. Email: natanael_moreno@yahoo.com Cel: +52 1 644 114 6750
On April 27, 2016, Arif Khan wrote:
Dear brothers: I am Arif from Kabul Afghanistan. i am an engineer with enough experience, I wanted to start a battery recycling company in Kabul but i dont have enough information about battery recycling so i wanted to know about the process, costs and other expenses and if any one wants to take a partner ship. Please email or you can call me at any time. Best regards Email: arif.ahmadzai@gmail.com Cell #: +93799033111 +93744889111 Skype: arif.ahmadzai786
On April 26, 2016, Oliver Abara wrote:
Dear Sir, I am into Lead /scrap battery export, I am based in Nigeria and Benin republic. Any interested buyer, individual or company should please contact me. email: oliver12abara@gmail.com
On April 26, 2016, Debaraj Mishra wrote:
Is anybody interested for lithium ion battery exporting. We are here in South Korea follows the complete recovery of product from LIB waste battery. We do receive batteries from Japan, US and some other places. If anyone from Europe would be interested to recycle LIB, we would be please do so. Thanks and regards.
On April 26, 2016, Azim khan wrote:
Email;; azim9750@gmail.com ,
On April 26, 2016, Azim khan wrote:
My contact number 9738764268; 9738434739
On April 26, 2016, Azim khan wrote:
Sir , I m from Karnataka , so I needed ur help to set up a new recycling plant , but her thier is no shortage of batteries , so I want to start new plant
On April 22, 2016, Lokesh Tripathi wrote:
Dear Sir, How are you! Glad to know that you want to set up a plant related to recycling, I like to introduce myself as a Manufacturer of special purpose machinery related to recycling and setting up existing plant in more economical manner. Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market of $33 billion, lead acid (Car Battery) is the most common battery in use. As per the battery chemistry Lead Acid market value per ton is equal to $1500 which is highly profitable venture to start up also it remains the most suitable battery to recycle; 70% of its weight contains reusable lead. Now as per my understanding you want to recycle 10 tons of car battery per day right! We recommend 03 tons of Rotary Furnace with pollution control equipment keeping environment as a necessary aspect. Whole process will work like this: Stock of Used Car Battery -> to the battery cutting machine -> desulphurisation of acid from lead -> desulphurised lead sent to furnace -> ingot bullion casted -> sent to refining kettle furnace -> Refined Lead is stacked in Ingot Casting Conveyor. Our Innovative technology, Design, Precise workmanship, Prompt after sale service has edge to meet demands of today’s industry. The turnkey capabilities allow us to support our client with any types of job from relining Containers to major installations Should you however need any additional information or clarification in process of finalizing the above 0requirement. Please call us or write to us. Mean while thanking you & assuring you best of our services at all the times to come. We remain… Your prompt reply shall be highly appreciated. Please contact Me: Name : Lokesh Tripathi PH:0091- 9711141615 Location : India , Delhi, (NCR) Email: info@indotherm.co.in
On April 8, 2016, Debaraj Mishra wrote:
Hi I have been working LIB recycling for last five years in S Korea Here recycling has heavy demand. I would like to start similar in India. I know the technology but major problem in India is to collect the battery material. Anybody would join with me in collection process so that I can think about the detail recycling process, starting from manual sorting, mechanical crushing and final product making by hydro process? Do mail me debraj.mishra@gmail.com. Thanks
On March 28, 2016, Naveed Shaikh wrote:
To introduce ourselves, we are a 30 year Old Company based in Mumbai, India in the field of Lead Oxides, Lead Battery Recycling & Battery Manufacturing .We are manufacturers of these equipment and undertake such Projects on Turnkey basis. Consultancy is also a part of our service. Our Company is a team of Well Experienced technocrats who have experience of more than 35 years Individually. We have executed projects in Indian Sub Continent, Middle East, Africa, Far East and Russia. sales@acsleadtech.com +91-9987077382
On February 29, 2016, Oneal Lajuwomi wrote:
Dear All, Our organisation has reached a decision to diversify and enter a new market, which is recycling and manufacturing of lead acid batteries in Nigeria, we are in search of an expert in the sector to help us achieve our dream of a fully functional factory for production of lead acid recycling and manufacturing of batteries. We will appreciate if you can assist us with a detailed machinery costing of setting up a Small-Medium factory that can produce between 500 -1000 lead acid batteries per/day, installation, commissioning cost, land size requirement and plan of action. I look forward to hearing from you. my email is oneal@wavelengthips.com
On February 22, 2016, ABDOU KADER SONKO wrote:
is it possible to get all the informations in french version? Aniway i am very interesting about batteriesrecycling,i start it already with a netherland friend in my country SENEGAL WEST AFRICA. THANKS
On February 11, 2016, Saras wrote:
Hi guys, I want some idea on the salvage value of a used Li-ion battery ( batteries that are expired after electric car usage )
On February 9, 2016, Ganesh wrote:
I am interested.can anybody help me in detailed.l am from Maharashtra. Mr. Imran l would like to listen from you.so plz give me your no. And plz tell me when should i call. Thanks Ganesh 09822430709
On January 30, 2016, Sridhar wrote:
Dear Friends, Can anybody tell what'll be the weight loss when lead from scrap batteries are melted? Regards Sridhar e-mail: taraneil123@gmail.com
On January 26, 2016, Ali Azam wrote:
Dear Sir You are welcome if you are setup factory in our Country (Bangladesh) Thank you Regards Email: aliazam09@gmail.com
On January 20, 2016, Kenneth Dumelo wrote:
We have Drained Battery Scrap and Aluminum, available for immediate supply to any serious buyer. If you are interested in any of these scrap materials, or have a buyer interested and ready to Purchase, kindly let us know. Best Regards Mr. Kenneth Dumelo Skype: zuruithinternational11 +233-279006232
On January 20, 2016, Imran khan wrote:
Hi Nicky, Please find my email id imran.r3999@gmail.com Thanks Imran
On January 20, 2016, Hushen kKafi wrote:
I am interested in this field, i am from (Gujarat) India, I am looking to start scrap battery business. Please help me 919723322170
On December 27, 2015, manoj kumar wrote:
hi all i am looking to start battery scrap and e waste scrap business in punjab ...india please help me if anyone can ....thnx ...... manoj gupta +919646099343
On December 9, 2015, Nickey wrote:
Hi, Imran Khan, Can you share your email id with me? Thanks Regards Nickey
On December 9, 2015, Imran wrote:
Hi Nicky, You can feel free to call me for more information Thanks Imran Khan Global lead alloys +918123561118
On December 9, 2015, Nickey wrote:
I am Nickey from China. I am very interested in this business. I wanted to start this business in China. but my information or knowledge is not enough to run it..anyone can share information or help. Thanks Regards Nickey
On November 30, 2015, darius wrote:
Battery Chemistry Metal value (per ton) Table 1: Metal value per ton of battery Lithium cobalt oxide $25,000 My Dear Friends, I have joined this tread months ago and it looks like to be a bug in pricing of used Lithium Cobalt Oxide batteries/ cells. Price tag should be $2.500 is $25.000 If I am wrong, pls correct me and let me to identify type of used batteries priced so high on a market. How these batteries are marked in printed symbols ? If you are interested I can arrange sample deliveries of any type of used batteries from Europe. thank you darius
On November 30, 2015, Sunny Alappat wrote:
Please contact me for information by email s.alappat @ ebnltd.com
On November 30, 2015, George Englezos wrote:
Interested to set up a recycle plant in Middle East. Any fusibility study you have available will be very helpful to me
On November 12, 2015, Arif Khan wrote:
Dear brothers: I am Arif from Kabul Afghanistan. i am an engineer with enough experience, I wanted to start a battery recycling company in Kabul so i wanted to know about the process, costs and other expenses and if you can take a partner ship. Please email or you can call me at any time. Best regards Email: arif.ahmadzai@gmail.com Cell #: +93799033111 +93744889111
On October 9, 2015, Sunny Alappat wrote:
We are interested to buy Scrap batteries from Nigeria. If anyone has the availability to quote their best offer by email. Thanks,
On September 26, 2015, Mohan Rajan wrote:
A low cost unit to process / Recycle SCRAP BATTERIES - other than lead Acid / Dry lead Acid batteries, can be established in India at Export Processing Zone. We can establish and operate such a unit, to process 20 MT / Monthly of Zn Carbon / Alkaline batteries. Other batteries can be processed in small quantities. All process with be by manual separation using hand operated tools and Melting of Non Ferrous metals. Investors / Scrap battery Exporters interested in joing us in setting up the proposed unit can contact Mohan Rajan E mail : mohraj1@rediff.com
On August 23, 2015, Przemek wrote:
Hi, could anyone share some information about used batteries transportation? As it's a hazardous material i think it may not be that easy to deliver it to any recycling point in another country.... or am i wrong? przemyslawrzosek@gmail.com
On August 21, 2015, Saurabh wrote:
Would like to understand recycling ecosystem
On August 18, 2015, darius wrote:
Hello Alyssa, please email me manta103g@gmail.com I would like to integrate your interest in battery recycling with my expertize in giving used batteries a second Life, developing LED + solar PV module + used battery kits for the Poor families in Africa. manta103g@gmail.com
On August 18, 2015, darius wrote:
Hello Alyssa, please email me I would like to integrate your interest in battery recycling with my expertize in giving used batteries a second Life, developing LED + solar PV module + used battery kits for the Poor families in Africa. manta103g@gmail.com
On August 18, 2015, Alyssa J wrote:
I recently just started to work at a landfill here in central Texas. I have been collecting all sorts of batteries that are dumped here at the landfill daily. I have been doing my research in battery recycling. If anyone is interested in trying to make a profit out of this with me please contact me. 254-316-8593
On July 15, 2015, Ravin wrote:
Hi all Looking a job in battery recycling industry with very good experience of smelting section. +91 8502051920
On July 4, 2015, Lee wrote:
Hi All, We're looking to start a reconditioned battery factory in Malaysia. We're looking for a consultant who can help us set up. References would be helpful particularly Malaysian references. Thank you. I can be contacted at uklee330@yahoo.com
On July 3, 2015, Lee wrote:
Dear Imran, We are interested in starting a reconditioned battery plant in Malaysia. Have you consulted with any Malaysian companies? Can I have their contacts so that we can obtain references from them. Thank you. You can contact me at uklee330@yahoo.com
On June 17, 2015, Dan Moore wrote:
I can recycle industrial NiCd batteries cheap from US only, email me dan@hrslater.com
On May 1, 2015, Andy Hurst wrote:
where is the best place to get recycled laptop batteries
On February 25, 2015, imran wrote:
Hi snoop, call me will discuss. Regards, Imrankhan +918123561118
On February 24, 2015, anoopkumar wrote:
I am interested this budiness.i am indian now from qatar any adviceand idea give me to start the budiness
On February 21, 2015, Adeleke Solomon Michael wrote:
Sir, I live in nigeria. I have the capacity to export drain scrap batteries to any countries. Please I need a serious buyer. Contact me. Micsteelum38@yahoo.com. 2348033067039, 2348023292444 .
On February 4, 2015, s.m wrote:
hi please help me about Absorbent devices manufacturer of lithium from seawater.
On January 6, 2015, AGray wrote:
I am involved in recycling batteries as part of a contest with school children. Is there any way outside of family use that we can gather large numbers of recycled batteries (in UK)? Is it ok to take them from say recycling points in supermarkets? They are all going to the same place right?
On December 8, 2014, imran khan wrote:
Hi AJYoung Please call me for more information regarding recycle of battery. Thanks, Imran +918123561118
On November 11, 2014, AJ YONG wrote:
Hi all...i have start plaining to do a recycle business for cell phone in malaysia...but i need more information or knowledge to run it..anyone can share information or help... Thank you..
On October 28, 2014, Fauz khan wrote:
I start to setup my own Recycle industry in India.if anyone who interested then plz koi with me.... Contact-09893613445
On September 4, 2014, Mike wrote:
I want to be buying used cell phone batteries for overseas export. I want bulk quantity purchase in 1000s for select cell phone batteries. Does anybody have any idea of companies that recycle cell phone batteries? Please help
On August 18, 2014, Kenneth Dumelo wrote:
kennethdumelo1@gmail.com
On August 18, 2014, imran.r wrote:
Hi Dumelo, can you share your email id..please Thanks Imrankhan +918123561118
On August 18, 2014, Kenneth Dumelo wrote:
Dear Sir We have Drained Battery Scrap, Used Rails, and, available for immediate supply to any serious buyer. If you are interested in any of these scrap materials, or have a buyer interested and ready to Purchase, kindly let us know for more details. Best Regards Mr. Kenneth Dumelo +233-260-930-922
On July 23, 2014, imran.r wrote:
@nouman - you call my number will let you in details. +918123561118
On July 23, 2014, nouman wrote:
please send be fesiblity report and tell me good suggestion i m intersted in battery recycling or car used battery recycling , thanking you
On June 25, 2014, imran.r wrote:
Hi George, My website address: www.globalleadalloys.com feel free to contact me. Imrankhan +918123561118
On June 25, 2014, imran wrote:
Hi akshay, It's easy for set up lead recycling plant with pollution control devices but without hazardous and pollution control board license you can't run the plant.. getting those license is not possible one. I have my own lead recycling plant with licences also import of batteries and rail materials. If any one intrested for business partner please consider this as my proposal. Please find my company website below. Www.globalleadalloys.com
On June 25, 2014, george stavropoulos wrote:
Hello, i am interested in this project, can i ask some question? About how large is this global market right now (in money terms)? To answer this one may need to know just the global market of batteries sold (tonnes and/or euros), the quantity and price of recovered metals can be derived. Thanks in advance, George
On March 18, 2014, akshay thote wrote:
We have regular requirement for lead acid battery scrap, we are looking for reliable supplier for long-term business relation. We also can help people to set-up a Battery recycling plant with pollution control devices. Please do not hesitate to contact me on my email id: sales@metalint.co.in
On December 13, 2013, Mirza Abrar wrote:
we have lead acid battery regenerating plant newly installed himself; and also intrusted to expand it in pakistan . this unit is state of the art technology which is developed in current year. production depends upon the istalled units.
On November 14, 2013, Razdar Muhammad wrote:
plz contect me on +92 346 9715441
On November 14, 2013, Razdar Muhammad wrote:
Hi, i want to start a cell phone batteries manufacturing business in pakistan. please help me. plz plz plzzzzzzzzzzzzz
On November 3, 2013, Imran R wrote:
Hai, I have my own battery lead recycle factory with all govt certificates.located in krishnagiri tamilnadu ,India...I am looking for partner for my business. You can feel free to contact. 919341836119 918123561118 Contact person name: Imran
On October 20, 2013, TCB wrote:
To: Carlos Carboni please contact us: trade @ tcbaltic . eu
On October 20, 2013, Carlos Carboni wrote:
I am interested in exporting disposed lead acid batteries from Costa Rica. Shipments would include automotive batteries without the electrolyte and sealed VRLA batteries such as those used in uniterruptible power supplies and other non-automotive applications. I may ship up to two 20 Foot containers per week with an average load of 20.000 Kgs. In the past I was involved in an organization that shipped similar quantities to several destinations in Asia. I would like to help clean the environment of my home country while making some money!
On October 9, 2013, Ernesto Hernandez wrote:
I want to start my own recycling center here in Perris, CA i want to know want i need to start and how muck are you guys pay per lb on the batteries. If you can get back to me i will appreciate it thanks
On October 7, 2013, levan wrote:
I am writing from Georgia and I'm doing toner cartridges recycling plant as well as printers and other computer equipment repair maintenance, our country is not a battery recycling   Enterprise. Please help me where is the recycling center because it will take part in nature conservation. Thank you
On September 18, 2013, Kushle Sharma wrote:
I want to start Acid Battery Recycling Industry in Jaipur,Rajasthan,India. I dnt kno d process dat how to start lead business? Can anyone help me to start d process of industry?
On July 5, 2013, Barbara Barron wrote:
I also am interested in battery recycling and would like to be kept informed of any updates to the present info.
On May 3, 2013, S.Rytis wrote:
Hello Mr.Scott at the moment our company looking for trusted partner, that to properly manage battery scrap business in UK. If you are intrested, please contacts us: trade (at) tcbaltic.eu Regards S.Rytis
On May 3, 2013, Dan Scott wrote:
I am interested in this field, I am from the UK, much seems a gap in the market here for this still. I would appreciate any help and support to help me get started.
On March 12, 2013, Ed wrote:
I would urge those who are considering business models based on battery "recycling"—that is, recovering batteries' constituent components and materials for resale at a profit—to think very hard first. Then, think about it some more. The essence of the article is that NiMH battery recycling might just break even, and only automotive lead-acid battery recycling is profitable in any meaningful way. Other battery types involve too much labour and energy to be recycled without subsidies. I know that in North America, product- and battery-manufacturer-subsidized programs exist to pick up and recycle these types. Check your local listings. I would expect Europe to offer similar or better options. You would be well advised to make use of these programs because you will only lose money doing it yourself without a subsidy. If you're really determined, you might set up a facility and join one of these programs yourself, but that seems like a poor idea for a stand-alone business. I don't think you could really profit in this way; instead, it would likely be a part of a larger, profitable, operation If you have large quantities of marginal batteries, you might find useful the equipment manufactured and sold by Cadex Electronics, the creator and host of Battery University. Such equipment includes battery analyzers, testers, and reconditioners for various cell types. You might save enough money by restoring and returning batteries to service rather than discarding them, for the equipment to pay for itself. I want to point out that storing large numbers of lithium-ion batteries is potentially dangerous. You do not simply throw these into a big pile and turn your back if you know what's good for you. It's not too hard to imagine a short circuit occurring, due perhaps to a conductive area on a battery casing, or some random piece of metal dropped into the pile. The next thing you know, you have a toxic lithium fire that you can't put out (hint: DO NOT use water!). The larger the pile, the greater the danger, kids. Precautions include carefully storing batteries to prevent short circuits, isolating them from flammable materials (including other batteries), and discharging them prior to storage. People view lead-acid batteries as toxic waste that should be disposed of at cost, so many leave their non-working automotive batteries laying about in random parking lots and industrial areas by the dark of night. However, many metal-recycling facilities will accept lead-acid batteries, paying perhaps $10 for an automotive battery. Most people seem to be unaware that you can be paid for your old battery. A bonus is that the toxic lead is kept out of the environment. There appears to be an opportunity for a business recycling the lead-acid battery. Some batteries might be obtained at little to no cost, so the profit potential seems significant. However, the toxic nature of the activity means that you are limited in where this could be done, and it seems it would be part of a larger and profitable metal-recycling operation. You will not be doing this in your back yard. A theme appears to be developing: a stand-alone business accepting batteries for recycling seems hopeless. The Cadex equipment, however, might be useful in reducing costs for operations that already have large quantities of poorly functioning rechargeable batteries for whatever reason. Examples of such operations might include industrial battery users trying to minimize battery replacement costs, and recycling operations trying to divert some batteries for reuse rather than being recycled, thus (perhaps) paying for the equipment. Like Cadex, I am in the Vancouver area, but that is a coincidence. I have nothing to do with Cadex except that I am a fan of Battery University, so I do not know how much the equipment costs or how long it would take to pay for itself. I suspect the man on the street would have to be very patient and start young. Finally, I can't help remarking on the previous comment by "lb gragg." It was my original intent, but I got off the rails. Gragg, the fact that you ask such a question about how God "stores" electricity is almost comical in its irony, for gods are not known for encouraging questions. However, in your unconventional writing style, you appear to be describing two things, both of which exist here on Earth (come down and join us): 1) Capacitors, and 2) Electric railroads. Both old news. If you would devote as much time to studying scientific literature or even the Wikipedia as you do religious texts, you would have known this. Cheers.
On January 17, 2013, lb gragg wrote:
It seems to me there should be a better way to store electricity how did God do it to make lightning maybe someone has or will If the road or something else was pos or neg and the other was mechanically produced with movement and a start primer little battery storage needs also the carrier line could steer the car
On November 14, 2012, John Thompson wrote:
I have a continues supply of small spent 3.7v li-ion batteries that are piling up, I'm looking for a profitable recycling solution. vr4boostin@aol.com
On September 3, 2012, Rytis wrote:
We are looking for person who can help to set up the lead battery recycling business. We are very interested to open battery recycling factory in eastern Europe. If you able to help us please dont hesitate to contact. Regards
On August 20, 2012, Mark Batt wrote:
I am very interested the battery technology field, as I have worked with batteries for thirty years. and would like to advance my knowlegde, as to ways to make a profit instead of always breaking even.
On May 13, 2012, Bill Norcutt wrote:
I am spending time and resources developing a battery recycling----- Rare Earth Metal business Lookingt for and offering help to others Bill Norcutt dollarbillsdallas@tx.rr.com 214-264-9000
On February 10, 2012, Ziv Lang wrote:
Do you have information pertaining to the actual recycling sites situated in the aforementioned countries?