BU-201b: Gel Lead Acid Battery

Learn the unique advantages of lead acid batteries

The early gelled lead acid battery developed in the 1950s by Sonnenschein (Germany) became popular in the 1970s. Mixing sulfuric acid with a silica-gelling agent converts liquid electrolyte into a semi-stiff paste to make the gel maintenance free. The AGM that arrived in the early 1980s offers similar performance to gel but each system offers slightly different characteristics to fill unique market needs. Gel batteries are commonly used in UPS, big and small, while AGM has carved out a market with starter and deep-cycle applications. Gel and AGM batteries are part of the valve-regulated lead acid (VRLA) family to make the traditional flooded lead acid maintenance free.

Energy storage systems (ESS) deployed for frequency regulation and energy buffering use lithium-ion batteries. Unlike lead acid, Li-ion can be rapid charged when excess energy is available. While UPS normally dwells at full-charge and is only discharged occasionally, Li-ion in an ESS can operate at mid-state-of-charge of 40 to 60 percent without inducing sulfation. UPS for standby applications continue to be served by lead acid batteries because of economical cost, ruggedness and superior safety, Li-ion is making inroads into applications that need cycling by delivering the best price per cycle.

A gel battery generally lasts longer than AGM; improved heat transfer to the outside is one reason. (The gel separator moves heat whereas the absorbent glass mat of the AGM acts as insulator.) A further advantage of gel is the dome shaped performance curve that allows the battery to stay in the high performance range during most of its service life before dropping rapidly towards the end of life; AGM, in comparison, fades gradually.

Gel is known for good performance at high ambient temperatures, is less prone to sulfation than other systems, but it needs the correct charge and float voltages. In comparison, AGM is superior at low temperatures with better current delivery because of low internal resistance. The cycle count on gel is said to be larger than AGM and the secret lies in holding more acid due to its design. Because of higher internals resistance, gel batteries are not used for high current applications.

One of the secrets of building a good gel battery lies in the valve construction. Small and economical gel batteries use a valve consisting of EPDM-rubber (EPDM stands for ethylene propylene diene monomer). High quality large gel batteries for use in high and low temperatures use a more elaborate valve design to improve moisture retention.

In terms of suitability and cost, the flooded lead acid is most durable when used in standby operation, but it is also the most expensive and requires maintenance by replenishing water. Gel is cheaper than flooded and is the preferred battery for the UPS installations in communications. AGM comes at a lower cost and is also superior in load capabilities to gel. Both systems have a promising future and will continue to serve for standby applications that require limited deep cycling. Table 1 illustrates the advantages and disadvantages of the gel battery over other lead acid systems.
 

Advantages Maintenance free; can be mounted sideways; low self-discharge
  Long lasting due to its ability to transfer heat to the outside
  Performance stays high until the end of life, then drops rapidly
  Produces water by combining oxygen and hydrogen
  Safe operation and forgiving if abused; less dry-out than AGM
  High cycle count, tolerance to abuse and heat
  Large variety of battery sizes available
Limitations Higher manufacturing cost than AGM 
  Sensitive to overcharging (gel is more tolerant than AGM)
  Moderate specific energy and load current
  Subject to release gases. Ventilation needed
  Must be stored in charged condition (less critical than flooded)

Table 1: Advantages and limitations of the gel battery.

Last updated 2017-10-11
 

 

*** Please Read Regarding Comments ***

Comments are intended for "commenting," an open discussion amongst site visitors. Battery University monitors the comments and understands the importance of expressing perspectives and opinions in a shared forum. However, all communication must be done with the use of appropriate language and the avoidance of spam and discrimination.

If you have a suggestion or would like to report an error, please use the "contact us" form or email us at: BatteryU@cadex.com.  We like to hear from you but we cannot answer all inquiries. We recommend posting your question in the comment sections for the Battery University Group (BUG) to share.

Or Jump To A Different Article

Basics You Should Know
The Battery and You
Batteries as Power Source

Comments (4)

On June 28, 2017 at 7:04am
Remco Schrijver wrote:

This is a very usefull website. Thank your for making this possible. In reading this piece however there are some things that are not correct if I may be so bold.

Gel was invented in the mid 1950’s by the Sonnenschein factory, AGM is invented later on. AGM batteries are commonly used in UPS systems, big and small. Not GEL.

Gel is used in deepcycle applications, however AGM is gaining marketshare in that same area due to lower costs and higher specific energy. Please note that there is a difference between UPS and Deep cycle AGM batteries. Not all AGM is desgined for cyclic application.

AGM is more sensitive to overcharging in comparance to GEL. Gel is more ;;robust’’ and can take abuse better. AGM performes better in cold conditions and GEL performces better in higher temperature surroundings. These days there are GEL batteries specially designed for high temperature surroundings (DEKA Fahrenheit for instance).

One of the reasons GEL can do more cycles lies in the additive of fosforic acid and the ability to hold more acid due to its design.

On July 16, 2017 at 9:39am
Joe Chau wrote:

Thanks for this good info article. Is “but cheaper than flooded” mentioned in the Limitation section might a typo? It is often said that Flooded Lead Acid is the cheapest of AGM and Gel. Are we talking about some special type of flooded that is also VRLA? Also “Vale-regulated Lead Acid” near the end of the first paragraph is a typo.

On December 21, 2017 at 5:55am
Al Mamun wrote:

Dear, as i read somewhere that, Sealed Maintenance free batteries are like dead when their charge level drops to less than 40%. Means these batteries cannot give full power by recharge, if they are reached to 40% of their capacity. Is it true?

On May 10, 2018 at 8:22pm
hung wrote:

Tôi rât thic trang we nay