Tweaking the Mobile Phone Battery

There are more mobile phones in the world than people. No other products have taken off so quickly — faster than the automobile, television, the PC and the Internet. Advancing from a clunky and expensive box in the 1990s to a sleek touchscreen device, the mobile phone still has one troubling component; the battery. Improvements have not been as fast on the battery as with other developments and credit for long runtime goes mostly to advancements in electronics, software and infrastructure.
 

A mobile phone battery must meet two requirements: High specific energy (capacity) and high specific power. Capacity refers to energy storage (Ah) analogous to the water in a bottle; specific power reflects in the ability to deliver current (A) representing the mouth opening of the bottle. Figure 1 demonstrates the relationship in the form of a water bottle.

A mobile phone battery needs high capacity and reasonably good specific power. These are two unique attributes that cannot be put into one product without compromise. An analogy is political parties that pursue different mandates and must make a compromise. In the battery, specific energy is responsible for runtimes and specific power for current.

Figure 1: Relationship between specific
energy and specific power.

 


The early Li-ion battery of the 1990s was fragile and unsuitable for high loads. This delayed the use of Li-ion in power tools and electric vehicles. These markets were reserved for the more rugged nickel-cadmium and later nickel-metal-hydride. Today lithium-based systems stand shoulder to shoulder with nickel and lead chemistries. This was made possible with the development of two types of Li-ion systems; the Energy Cell delivering maximum runtime and the Power Cell enabling heavy loading.
 

Energy Cell

The Li-ion Energy Cell has a high ampere-hours (Ah) rating for long runtimes and the Panasonic NCR18650B illustrated in Figure 2 is such a product. This cell delivers a capacity of 3,200mAh when discharged at 0.5C or 1.6A. The battery is delicate in that the capacity decreases to 2,300mAh when discharging at 2C or 6.4A. For purpose of analysis, the end-of-charge is set to 3.0V; the cutoff is marked with the red circle. (Ampere-hours with smaller batteries are given usually in milliampere-hours (mAh).)

The end-of-discharge cutoff for many devices, including the mobile phone, is often above the designated 3.0V; 3.3V is common. This reduces the usable capacity, especially if discharged at a high current. In many mobile phones, 3.3V refers to zero charge. Some phone may keep operating, others will close shop. Voltage recovery may allow short uses after a rest or when keeping the phone warm.

 

18650
Figure 2: Discharge of 3,200mAh Energy Cell
Panasonic NCR18650B is discharged at 0.2C, 0.5C, 1C and 2C. The red circle marks early cutoff at 2C.
Cold temperature losses:
25°C (77°F)  = 100%
0°C (32°F)    = ~83%
–10°C (14°F) = ~66%
–20°C (4°F)   = ~53%
Source: Panasonic


The Energy Cell should not be fast-charged at a higher rate than 1C; 0.8C or less is recommended to achieve the specified cycle count. Loading above 1C also adds stress, reflecting in reduced longevity. This cell is ideal for portable computing and mobile phone applications with light to moderate loading requiring long runtimes.


Power Cell

The Panasonic UR18650RX Power Cell in Figure 3 has a capacity that is 40% less than the Energy Cell, but has excellent loading capabilities. A 10A (5C) discharge has minimal capacity loss when referring to the 3.0V cutoff. This cell works well for applications requiring heavy load current, such as power tools.
 

18650
Figure 3: Discharge of 1,950mAh Power Cell.
Panasonic UR18650RX is discharged at 0.2C, 0.5C, 1C and 2C and 10A, reaching the 3.0V/cell cut-off line at about 2000mAh in the red circle.
Cold temperature losses:
25°C (77°F)  = 100%
0°C (32°F)    = ~92%
–10°C (14°F) = ~85%
–20°C (4°F)   = ~80%
Source: Panasonic


Further advantages of the Power Cell over the Energy Cell are faster charge times and improved low temperature performance. All batteries lose performance when cold but the Li-ion Power Cell overcomes this by providing 92% capacity at 0°C (32°F) and 80% at –20°C (4°F). In comparison, the Energy Cell drops to 83% at 0°C (32°F) and 53% at –20°C (4°F). Never charge Li-ion below freezing as this causes the plating of metallic lithium. This may go unnoticed but can compromise the safety of the battery.

The Power Cell achieves superior performance in part by optimizing the surface area of the active materials to enable high current flow with minimal temperature rise. Batteries for mobile phones are crossbred to achieve long runtime and provide the necessary loading capability during active use.
 

Relaxed Requirements

One of the major advantages of the mobile phone battery compared to other devices is the use of a single Li-ion cell. This simplifies the safety circuit and does not require cell matching as is necessary with multi-cell packs. This, however, opens the floodgates for broader performance tolerances. Most users would not notice a slightly shorter runtime of a battery that passes at the low-end of the bell curve.

Mobile phones come with built-in obsolescence to entice selling a new model when the battery fades or the glass cracks. Other products have stricter requirements in terms of battery longevity and the electric vehicle is an example. EV batteries are guaranteed for eight years; the replacement cost is as much as a regular economy car. Manufacturers can build batteries that last and much of this is achieved by avoiding full charges and complete discharges.

Mobile phones are made in large quantity and come with a customized pack. Standard sizes do not apply. Because of size restrictions the choices are most often prismatic or pouch. The popular 18650 cell finds applications in power tools, medical instruments, e-bikes and some EVs.

When the state-of-charge (SoC) gets low and the mobile phone approaches the cutoff voltage that is between 3.2–3.5V, the internal resistance of the battery rises. This causes the voltage drop further. The load current on a smartphone ranges from 0.6–1.9A. While talking may still be possible with low charge in close proximity to a tower, GPS and complex computing functions requiring higher operating current and the phone may cut off. Accessing a tower in a fringe area also requires more power than being in line-of-site. A bright display also consumes power. Table 4 estimates typical current consumptions of a modern smartphone.

 

Application Current draw
CPU usage low 200mA
CPU usage high 900mAh
Main camera active 200mAh
Front camera active 100mAh
WLAN enabled 50mA
LCD backlighting 100mAh
Total current draw 600 to 1,900mA

Figure 4: Current draw of a mobile phone.
Multiple applications are engaged when using our mobile phones that add to a total current draw for a given time. Some applications are momentary; others stay on as housekeeping functions.


Testing Mobile Phone Batteries

Capacity is the leading health indicator of a battery. Elevated internal resistance is also a failure mode but this is less common. Several methods can be used to estimate the state-of-health (SoH) of a battery.

Coulomb counting observes in and outflowing currents of a battery. The theory goes back 250 years when Charles-Augustin de Coulomb established the “Coulomb Rule” that equates one ampere (1A) per second as one coulomb. Coulomb counting measures the energy reserve and should give a fair estimation on the content. This method should be flawless but it has drawbacks. The energy drawn from the battery is always less than what is put in. Tracking errors occur by random use that accumulates over time. Coulomb counting works best when the phone is allowed to run down occasionally to enable calibration.

Apps are available to check battery SoH in mobile phones and laptops. This requires current sensing and not all mobile phones provide this feature. Experts examining the app method hint to inaccuracies. Cadex examined 20 batteries that had passed as good when tested with an app that was sold as a commercial product. Testing these batteries with a full cycle, the battery analyzer disclosed capacities ranging from 57–86% with internal resistance fluctuating from 155–368mOhm. With the capacity pass/fail threshold set to 80% and internal resistance to 200mOhm, only 5 of these 20 batteries would qualify for reusable.

Some mobile phone manufacturers include software tools that estimate battery SoH, but the readings are not made available to the general public and are only accessible to authorized personnel by security code. This is done for good reason. Making capacity readings available to the users could lead to high warranty claims, especially if the phones are not calibrated and the readings are skewed. A replacement is only mandatory if the battery capacity drops below 80 percent. Keeping the evidence hidden is least disruptive.

The most reliable method to check a battery is applying a full discharge cycle. Although time consuming, some refurbishing houses apply this method to get accurate readings with a printed performance report. With automated battery analyzers, the only labor is refilling the stations and the throughput is high. Storefront and small service centers prefer rapid test methods that give reasonable accurate results in just a few minutes. Rapid-testing takes a snapshot of the “chemical battery” rather than relying on the “digital battery” that is often fraught with tracking errors.

Most smartphones no longer provide access to the battery, but service centers and refurbishing houses still need to check them. This can be done by opening the devices and connecting the miniature connectors to the FlexStrip interface provided by the battery analyzer. Such work is no longer performed at storefront but by skilled technicians in a service environment.


References: W-Support GmbH, Germany. Axel Brandt

 

About the Author

Isidor Buchmann is the founder and CEO of Cadex Electronics Inc. For three decades, Buchmann has studied the behavior of rechargeable batteries in practical, everyday applications, has written award-winning articles including the best-selling book “Batteries in a Portable World,” now in its fourth edition. Cadex specializes in the design and manufacturing of battery chargers, analyzers and monitoring devices. For more information on batteries, visit www.batteryuniversity.com; product information is on www.cadex.com.
 

Last updated 2017-05-26


*** Please Read Regarding Comments ***

Comments are intended for "commenting," an open discussion amongst site visitors. Battery University monitors the comments and understands the importance of expressing perspectives and opinions in a shared forum. However, all communication must be done with the use of appropriate language and the avoidance of spam and discrimination.

If you have a suggestion or would like to report an error, please use the "contact us" form or email us at: BatteryU@cadex.com.  We like to hear from you but we cannot answer all inquiries. We recommend posting your question in the comment sections for the Battery University Group (BUG) to share.

Or Jump To A Different Article

Basics You Should Know
The Battery and You
Batteries as Power Source

Comments

On August 15, 2018 at 2:59pm
Martin wrote:

Hi, I own a 5300 mAh 2 months old mobile phone. It works fine. Battery lasts 4-5 days with not demanding usage.

Here the question. A full charge lasts one hour (1C). Charger is the original (rated 5V - 2.5A). But maths does not match. Charging in one hour that battery mean s 5.3A on average (it can be even higher first half of empty battery). I guess 5.3A current will kill the battery very fast.

Is it correct to charge a Li-Po at lower current rates?  I tried a lower current charger (5V - 1A) but charger got very hot.

Any idea about how to improve longevity in such phones?