BU-705a: Battery Recycling as a Business

Consider a new business but find out the return

Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market (2015) of $33 billion, lead acid is the most common battery in use. This is followed by Li-ion at $16.6 billion, NiMH at $2 billion and NiCd at $1 billion. All other chemistries only make up $1 billion. Table 1 lists the material cost per ton to build these batteries.
 

Battery Chemistry

Metal value (per ton)

Recycling

Table 1: Metal value per ton of battery.

Lead acid remains the most suitable battery to recycle; 70% of its weight contains reusable lead.

Lithium cobalt oxide

$25,000

Subsidy needed
Cobalt $50,000 (2017) Relevant, subsidy

Lithium iron phosphate

$400

Subsidy needed

Lead acid

$1,500

Profitable
Nickel $10,000–$17,000 Subsidy needed
Cadmium $2,200 Subsidy needed


Lithium-ion batteries are expensive to manufacture and this is in part due to the high material cost and complex preparation processes. The most expensive metal of most Li-ion is cobalt, a hard lustrous gray material that is also used to manufacture magnets and high-strength alloys.

Knowing that billions of Li-ion batteries are discarded every year and given the high cost of lithium cobalt oxide, salvaging precious metals should make economic sense and one wonders why so few companies recycle these batteries.

The reason becomes clear when examining the complexity and low yield of recycling. The retrieved raw material barely pays for labor, which includes collection, transport, sorting into batteries chemistries, shredding, separation of metallic and non-metallic materials, neutralizing hazardous substances, smelting, and purification of the recovered metals.

Recycling programs for lead acid are believed to have started soon after Cadillac introduced the cranking motor in 1912 as a for-profit business rather than protecting the environment. Recycling can be harmful, especially with lead acid batteries. Lead can enter the body by inhaling or ingestion when touching the mouth with lead-contaminated hands. This puts workers and residents of the surrounding areas at risk of lead poisoning. ( See BU-703: Health Concerns with Batteries )

The EPA (Environmental Protection Agency) has imposed strict guidelines in recycling of lead acid batteries in the USA. The recycling plants must be sealed and the smokestacks fitted with scrubbers. To check for possible escape of lead particles, the plant perimeter must be surrounded with lead-monitoring devices. Rules are bound to be broken and batteries soon end up in Mexico and other developing countries with relaxed regulations. China, a leader in lead acid battery production, also took action to protect the environment by introducing strict guidelines that only reputable companies can meet.

Nickel-based batteries can also be recycled and the retrieved materials are iron and nickel, which are used in stainless steel production. Nickel-metal-hydride (NiMH) yields the highest return in nickel, and with ample supply recycling is said to make money. Low demand for cadmium has reduced the profitability from recycling NiCd batteries. The growth in batteries is with Li-ion but valuable materials are difficult to retrieve. This makes Li-ion less attractive for recycling and a financial breakeven may not be possible without subsidies.

The true cost to manufacture Li-ion is not so much in the raw materials, as is the case with lead acid and NiMH, but in lengthy processing and purification processes of the raw materials to reach battery grade. Retrieving lithium at only 3 percent of the cell mix may never reach break-even levels. If the purity of lithium is below 99.5 percent, then it is not suitable as raw material for batteries. Recycling brings the metal to ground zero, from which costly preparations begin anew. It is often cheaper to mine raw material than to retrieve it from recycling. Lithium from recycled batteries is commonly used for non-battery applications, such as lubricating greases that are found in WD-40 and other products, rather than batteries. ( See BU-308: Availability of Lithium )

Although alkaline and zinc-carbon account for over 90 percent of batteries consumed in the United States, they contain few precious metals and the toxicity is low. Organizations are seeking ways to recycle these batteries as well for the basic metal content and with high volume such a venture should become viable. Table 2 lists the typical metals content of commonly recycled batteries.
 

 

Fe
Iron

Mn Manganese

Ni
Nickel

Zn
Zinc

Li
Lithium

Cd
Cadmium

Co
Cobalt

Al
Aluminum

Pb
Lead

Lead acid

 

 

 

 

 

 

 

 

65%

NiCd

35%

 

22%

 

 

15%

 

 

 

NiMH

20%

1%

35

1%

 

 

4%

 

 

Li-ion

22%

 

 

 

3%

 

18%

5%

 

Alkaline

24%

22%

 

15%

 

 

 

 

 

Table 2: Metals in commonly recycled batteries as a percentage of the overall content. The metal content may vary with battery type. With the exception of lead acid, most recycling requires a subsidy.
 

Facts about Battery Production and Recycling

Environmental issues and the ability to recycle play an important role when choosing a battery system. If the UPS operates mostly in standby and can provide longevity of 10 years, then lead acid is a strong contender. The preference of lead acid over Li-ion and nickel-based systems is manifested in moderate pricing, superior safety, dependable operation, and the ability to recycle. Table 3 compares the cost to manufacture and recycle batteries.
 

  Estimated cost of disposal Production process Carbon dioxide emission
Lead acid Profitable; lead has intrinsic value 30 mega joules; 8.3kW* 3kg per kg*
Lithium-ion $4,000–5,000 per ton 170 mega joules; 47kW* 12kg per kg*
NiCd, NiMH Can be cost neutral N/A N/A

Table 3: Costs of battery manufacturing and disposal.
* Quoted figures from Argonne National Laboratory
 

Summary

The primary objective of building a good battery is long life, safety and low price. Recycling is an afterthought and manufacturers do little to simplify the retrieving of precious metals. The recycling business is small compared to the vast battery industry, and to this day, only lead acid can be recycled profitably.

Nickel-based batteries might make money with good logistics, but Li-ion and most other chemistries yield too little in precious metals to make recycling a viable business without subsidies. The major expense with modern batteries is not so much the raw materials, as with lead acid, but lengthy preparations, purifications and processing down to micro- and nano-levels. Nevertheless, batteries contain valuable material that can be re-used for new products.

To make recycling feasible in the meantime, subsidies are created by adding a tax to each pack sold. The goal goes beyond retrieving metals for re-use to preventing toxic batteries from entering landfills. Combining the environmental benefit with making a profit is the ultimate goal, and this might become feasible with innovative new recycling processes in development.

Another model is to sort batteries into functional and non-functional groups and give those with capacities of 80 percent or more a second life. Cells and modules of larger battery systems can be tested individually and reassembled in a new pack. ( See BU-803: Can Batteries be Restored? )

Last updated 2018-03-29
 

*** Please Read Regarding Comments ***

Comments are intended for "commenting," an open discussion amongst site visitors. Battery University monitors the comments and understands the importance of expressing perspectives and opinions in a shared forum. However, all communication must be done with the use of appropriate language and the avoidance of spam and discrimination.

If you have a suggestion or would like to report an error, please use the "contact us" form or email us at: BatteryU@cadex.com.  We like to hear from you but we cannot answer all inquiries. We recommend posting your question in the comment sections for the Battery University Group (BUG) to share.

Or Jump To A Different Article

Basics You Should Know
The Battery and You
Batteries as Power Source

Comments (202)

On February 10, 2012 at 11:30am
Ziv Lang wrote:

Do you have information pertaining to the actual recycling sites situated in the aforementioned countries?

On May 13, 2012 at 6:01am
Bill Norcutt wrote:

I am spending time and resources developing a battery recycling——-
Rare Earth Metal business
Lookingt for and offering help to others
Bill Norcutt
dollarbillsdallas@tx.rr.com
214-264-9000

On August 19, 2012 at 10:37pm
Mark Batt wrote:

I am very interested the battery technology field, as I have worked with batteries for thirty years. and would like to advance my knowlegde, as to ways to make a profit instead of always breaking even.

On September 3, 2012 at 5:28am
Rytis wrote:

We are looking for person who can help to set up the lead battery recycling business. We are very interested to open battery recycling factory in eastern Europe. If you able to help us please dont hesitate to contact.

Regards

On November 14, 2012 at 12:45am
John Thompson wrote:

I have a continues supply of small spent 3.7v li-ion batteries that are piling up, I’m looking for a profitable recycling solution.
vr4boostin@aol.com

On January 17, 2013 at 4:44pm
lb gragg wrote:

It seems to me there should be a better way to store electricity how did God do it to make lightning maybe someone has or will If the road or something else was pos or neg and the other was mechanically produced with movement and a start primer little battery storage needs also the carrier line could steer the car

On March 11, 2013 at 6:06pm
Ed wrote:

I would urge those who are considering business models based on battery “recycling”—that is, recovering batteries’ constituent components and materials for resale at a profit—to think very hard first.  Then, think about it some more.

The essence of the article is that NiMH battery recycling might just break even, and only automotive lead-acid battery recycling is profitable in any meaningful way. Other battery types involve too much labour and energy to be recycled without subsidies.

I know that in North America, product- and battery-manufacturer-subsidized programs exist to pick up and recycle these types.  Check your local listings.  I would expect Europe to offer similar or better options.  You would be well advised to make use of these programs because you will only lose money doing it yourself without a subsidy.  If you’re really determined, you might set up a facility and join one of these programs yourself, but that seems like a poor idea for a stand-alone business.  I don’t think you could really profit in this way; instead, it would likely be a part of a larger, profitable, operation

If you have large quantities of marginal batteries, you might find useful the equipment manufactured and sold by Cadex Electronics, the creator and host of Battery University.  Such equipment includes battery analyzers, testers, and reconditioners for various cell types.  You might save enough money by restoring and returning batteries to service rather than discarding them, for the equipment to pay for itself.

I want to point out that storing large numbers of lithium-ion batteries is potentially dangerous.  You do not simply throw these into a big pile and turn your back if you know what’s good for you.  It’s not too hard to imagine a short circuit occurring, due perhaps to a conductive area on a battery casing, or some random piece of metal dropped into the pile.  The next thing you know, you have a toxic lithium fire that you can’t put out (hint: DO NOT use water!).  The larger the pile, the greater the danger, kids.  Precautions include carefully storing batteries to prevent short circuits, isolating them from flammable materials (including other batteries), and discharging them prior to storage.

People view lead-acid batteries as toxic waste that should be disposed of at cost, so many leave their non-working automotive batteries laying about in random parking lots and industrial areas by the dark of night.  However, many metal-recycling facilities will accept lead-acid batteries, paying perhaps $10 for an automotive battery.  Most people seem to be unaware that you can be paid for your old battery.  A bonus is that the toxic lead is kept out of the environment.

There appears to be an opportunity for a business recycling the lead-acid battery.  Some batteries might be obtained at little to no cost, so the profit potential seems significant.  However, the toxic nature of the activity means that you are limited in where this could be done, and it seems it would be part of a larger and profitable metal-recycling operation.  You will not be doing this in your back yard.

A theme appears to be developing: a stand-alone business accepting batteries for recycling seems hopeless.  The Cadex equipment, however, might be useful in reducing costs for operations that already have large quantities of poorly functioning rechargeable batteries for whatever reason.  Examples of such operations might include industrial battery users trying to minimize battery replacement costs, and recycling operations trying to divert some batteries for reuse rather than being recycled, thus (perhaps) paying for the equipment.

Like Cadex, I am in the Vancouver area, but that is a coincidence.  I have nothing to do with Cadex except that I am a fan of Battery University, so I do not know how much the equipment costs or how long it would take to pay for itself.  I suspect the man on the street would have to be very patient and start young.

Finally, I can’t help remarking on the previous comment by “lb gragg.” It was my original intent, but I got off the rails.  Gragg, the fact that you ask such a question about how God “stores” electricity is almost comical in its irony, for gods are not known for encouraging questions.  However, in your unconventional writing style, you appear to be describing two things, both of which exist here on Earth (come down and join us): 1) Capacitors, and 2) Electric railroads.  Both old news.  If you would devote as much time to studying scientific literature or even the Wikipedia as you do religious texts, you would have known this.  Cheers.

On May 3, 2013 at 2:50am
Dan Scott wrote:

I am interested in this field, I am from the UK, much seems a gap in the market here for this still. I would appreciate any help and support to help me get started.

On May 3, 2013 at 5:08am
S.Rytis wrote:

Hello Mr.Scott
at the moment our company looking for trusted partner, that to properly manage battery scrap business in UK. If you are intrested, please contacts us: trade (at) tcbaltic.eu


Regards
S.Rytis

On July 5, 2013 at 4:57am
Barbara Barron wrote:

I also am interested in battery recycling and would like to be kept informed of any updates to the present info.

On September 17, 2013 at 9:04pm
Kushle Sharma wrote:

I want to start Acid Battery Recycling Industry in Jaipur,Rajasthan,India.
I dnt kno d process dat how to start lead business?
Can anyone help me to start d process of industry?

On October 7, 2013 at 1:30am
levan wrote:

I am writing from Georgia and I’m doing toner cartridges recycling plant as well as printers and other computer equipment repair maintenance, our country is not a battery recycling
  Enterprise.
Please help me where is the recycling center because it will take part in nature conservation. Thank you

On October 9, 2013 at 1:45pm
Ernesto Hernandez wrote:

I want to start my own recycling center here in Perris, CA i want to know want i need to start and how muck are you guys pay per lb on the batteries. If you can get back to me i will appreciate it thanks

On October 19, 2013 at 10:36pm
Carlos Carboni wrote:

I am interested in exporting disposed lead acid batteries from Costa Rica. Shipments would include automotive batteries without the electrolyte and sealed VRLA batteries such as those used in uniterruptible power supplies and other non-automotive applications. I may ship up to two 20 Foot containers per week with an average load of 20.000 Kgs. In the past I was involved in an organization that shipped similar quantities to several destinations in Asia. I would like to help clean the environment of my home country while making some money!

On October 20, 2013 at 4:44am
TCB wrote:

To: Carlos Carboni
please contact us: trade @ tcbaltic . eu

On November 3, 2013 at 1:32am
Imran R wrote:

Hai,
I have my own battery lead recycle factory with all govt certificates.located in krishnagiri tamilnadu ,India…I am looking for partner for my business.
You can feel free to contact.
919341836119
918123561118
Contact person name: Imran

On November 14, 2013 at 8:19am
Razdar Muhammad wrote:

Hi,
i want to start a cell phone batteries manufacturing business in pakistan.
please help me. plz plz plzzzzzzzzzzzzz

On November 14, 2013 at 8:22am
Razdar Muhammad wrote:

plz contect me on +92 346 9715441

On December 13, 2013 at 8:15am
Mirza Abrar wrote:

we have lead acid battery regenerating plant newly installed himself;
and also intrusted to expand it in pakistan .
this unit is state of the art technology which is developed in current year.
production depends upon the istalled units.

On March 17, 2014 at 10:23pm
akshay thote wrote:

We have regular requirement for lead acid battery scrap, we are looking for reliable supplier for long-term business relation.

We also can help people to set-up a Battery recycling plant with pollution control devices.

Please do not hesitate to contact me on my email id: sales@metalint.co.in

On June 25, 2014 at 3:57am
george stavropoulos wrote:

Hello,
i am interested in this project, can i ask some question?

About how large is this global market right now (in money terms)?

To answer this one may need to know just the global market of batteries sold (tonnes and/or euros), the quantity and price of recovered metals can be derived.
Thanks in advance,
George

On June 25, 2014 at 11:06am
imran wrote:

Hi akshay,

It’s easy for set up lead recycling plant with pollution control devices but without hazardous and pollution control board license you can’t run the plant.. getting those license is not possible one.
I have my own lead recycling plant with licences also import of batteries and rail materials.


If any one intrested for business partner please consider this as my proposal. Please find my company website below.

Www.globalleadalloys.com

On June 25, 2014 at 11:10am
imran.r wrote:

Hi George,

My website address: www.globalleadalloys.com
feel free to contact me.

Imrankhan
+918123561118

On July 23, 2014 at 7:51am
nouman wrote:

please send be fesiblity report and tell me good suggestion i m intersted in battery recycling or car used battery recycling ,
thanking you

On July 23, 2014 at 9:43am
imran.r wrote:

@nouman - you call my number will let you in details.
+918123561118

On August 18, 2014 at 9:57am
Kenneth Dumelo wrote:

Dear Sir

We have Drained Battery Scrap, Used Rails, and, available for immediate supply to any serious buyer.

If you are interested in any of these scrap materials, or have a buyer interested and ready to Purchase, kindly let us know for more details.

Best Regards

Mr. Kenneth Dumelo
+233-260-930-922

On August 18, 2014 at 10:00am
imran.r wrote:

Hi Dumelo,

can you share your email id..please

Thanks
Imrankhan
+918123561118

On August 18, 2014 at 2:52pm
Kenneth Dumelo wrote:

kennethdumelo1@gmail.com

On September 3, 2014 at 7:36pm
Mike wrote:

I want to be buying used cell phone batteries for overseas export. I want bulk quantity purchase in 1000s for select cell phone batteries.  Does anybody have any idea of companies that recycle cell phone batteries?  Please help

On October 28, 2014 at 1:25am
Fauz khan wrote:

I start to setup my own Recycle industry in India.if anyone who interested then plz koi with me….

Contact-09893613445

On November 11, 2014 at 10:56am
AJ YONG wrote:

Hi all…i have start plaining to do a recycle business for cell phone in malaysia…but i need more information or knowledge to run it..anyone can share information or help…

Thank you..

On December 8, 2014 at 11:14am
imran khan wrote:

Hi AJYoung

Please call me for more information regarding recycle of battery.

Thanks,

Imran
+918123561118

On January 6, 2015 at 7:27am
AGray wrote:

I am involved in recycling batteries as part of a contest with school children. Is there any way outside of family use that we can gather large numbers of recycled batteries (in UK)?
Is it ok to take them from say recycling points in supermarkets?
They are all going to the same place right?

On February 3, 2015 at 5:07pm
s.m wrote:

hi
please help me about Absorbent devices manufacturer of lithium from seawater.

On February 21, 2015 at 1:46am
Adeleke Solomon Michael wrote:

Sir, I live in nigeria. I have the capacity to export drain scrap batteries to any countries. Please I need a serious buyer. Contact me. Micsteelum38@yahoo.com. 2348033067039, 2348023292444 .

On February 24, 2015 at 4:38am
anoopkumar wrote:

I am interested this budiness.i am indian now from qatar any adviceand idea give me to start the budiness

On February 24, 2015 at 7:25pm
imran wrote:

Hi snoop,

call me will discuss.

Regards,
Imrankhan
+918123561118

On May 1, 2015 at 4:02am
Andy Hurst wrote:

where is the best place to get recycled laptop batteries

On June 17, 2015 at 1:11pm
Dan Moore wrote:

I can recycle industrial NiCd batteries cheap from US only, email me dan@hrslater.com

On July 3, 2015 at 2:34am
Lee wrote:

Dear Imran,

We are interested in starting a reconditioned battery plant in Malaysia. Have you consulted with any Malaysian companies? Can I have their contacts so that we can obtain references from them. Thank you.

You can contact me at uklee330@yahoo.com

On July 3, 2015 at 6:20pm
Lee wrote:

Hi All, We’re looking to start a reconditioned battery factory in Malaysia. We’re looking for a consultant who can help us set up. References would be helpful particularly Malaysian references. Thank you. I can be contacted at uklee330@yahoo.com

On July 14, 2015 at 9:28pm
Ravin wrote:

Hi all
Looking a job in battery recycling industry with very good experience of smelting section. +91 8502051920

On August 18, 2015 at 6:35am
Alyssa J wrote:

I recently just started to work at a landfill here in central Texas. I have been collecting all sorts of batteries that are dumped here at the landfill daily. I have been doing my research in battery recycling. If anyone is interested in trying to make a profit out of this with me please contact me. 254-316-8593

On August 18, 2015 at 1:42pm
darius wrote:

Hello Alyssa,

please email me

I would like to integrate your interest in battery recycling with
my expertize in giving used batteries a second Life,
developing LED + solar PV module + used battery kits
for the Poor families in Africa.

manta103g@gmail.com

On August 18, 2015 at 1:44pm
darius wrote:

Hello Alyssa,

please email me

manta103g@gmail.com


I would like to integrate your interest in battery recycling with
my expertize in giving used batteries a second Life,
developing LED + solar PV module + used battery kits
for the Poor families in Africa.

manta103g@gmail.com

On August 20, 2015 at 6:55pm
Saurabh wrote:

Would like to understand recycling ecosystem

On August 22, 2015 at 5:08pm
Przemek wrote:

Hi, could anyone share some information about used batteries transportation? As it’s a hazardous material i think it may not be that easy to deliver it to any recycling point in another country…. or am i wrong? 

przemyslawrzosek@gmail.com

On September 26, 2015 at 1:11am
Mohan Rajan wrote:

A low cost unit to process / Recycle SCRAP BATTERIES - other than lead Acid / Dry lead Acid batteries, can be established in India at Export Processing Zone.

We can establish and operate such a unit, to process 20 MT / Monthly of Zn Carbon / Alkaline batteries. Other batteries can be processed in small quantities.

All process with be by manual separation using hand operated tools and Melting of Non Ferrous metals.

Investors / Scrap battery Exporters interested in joing us in setting up the proposed unit can contact

Mohan Rajan

E mail : mohraj1@rediff.com

On October 9, 2015 at 9:59am
Sunny Alappat wrote:

We are interested to buy Scrap batteries from Nigeria. If anyone has the availability to quote their best offer by email. Thanks,

On November 12, 2015 at 8:11am
Arif Khan wrote:

Dear brothers:
I am Arif from Kabul Afghanistan. i am an engineer with enough experience, I wanted to start a battery recycling company in Kabul so i wanted to know about the process, costs and other expenses and if you can take a partner ship.  Please email or you can call me at any time.

Best regards

Email: arif.ahmadzai@gmail.com
Cell #: +93799033111
        +93744889111

On November 30, 2015 at 3:18am
George Englezos wrote:

Interested to set up a recycle plant in Middle East.

Any fusibility study you have available will be very helpful to me

On November 30, 2015 at 3:27am
Sunny Alappat wrote:

Please contact me for information by email s.alappat @ ebnltd.com

On November 30, 2015 at 12:08pm
darius wrote:

Battery Chemistry
Metal value (per ton)
Table 1: Metal value per
ton of battery

Lithium cobalt oxide
$25,000

My Dear Friends,

I have joined this tread months ago and it looks like to be a bug
in pricing of used
Lithium Cobalt Oxide batteries/ cells.

Price tag should be $2.500
is $25.000

If I am wrong, pls correct me and let me to identify type of used batteries priced so high on a market.
How these batteries are marked in printed symbols ?

If you are interested I can arrange sample deliveries of
any type of used batteries from Europe.
thank you
darius

On December 9, 2015 at 2:14am
Nickey wrote:

  I am Nickey from China. I am very interested in this business. I wanted to start this business in China. but my information or knowledge is not enough to run it..anyone can share information or help. Thanks

Regards
Nickey

On December 9, 2015 at 4:20am
Imran wrote:

Hi Nicky,
You can feel free to call me for more information

Thanks
Imran Khan
Global lead alloys
+918123561118

On December 9, 2015 at 6:20am
Nickey wrote:

Hi, Imran Khan,
Can you share your email id with me?  Thanks

Regards
Nickey

On December 27, 2015 at 6:48am
manoj kumar wrote:

hi all
i am looking to start battery scrap and e waste scrap business in punjab ...india
please help me if anyone can ....thnx ......


manoj gupta
+919646099343

On January 19, 2016 at 8:59pm
Hushen kKafi wrote:

I am interested in this field, i am from (Gujarat) India, I am looking to start scrap battery business. Please help me
919723322170

On January 20, 2016 at 2:24am
Imran khan wrote:

Hi Nicky,

Please find my email id imran.r3999@gmail.com

Thanks
Imran

On January 20, 2016 at 12:27pm
Kenneth Dumelo wrote:

We have Drained Battery Scrap and Aluminum, available for immediate supply to any serious buyer.

If you are interested in any of these scrap materials, or have a buyer interested and ready to Purchase, kindly let us know.

Best Regards

Mr. Kenneth Dumelo

Skype: zuruithinternational11
+233-279006232

On January 26, 2016 at 3:01am
Ali Azam wrote:

Dear Sir
You are welcome if you are setup factory in our Country (Bangladesh)
Thank you
Regards
Email: aliazam09@gmail.com

On January 30, 2016 at 8:22am
Sridhar wrote:

Dear Friends,

Can anybody tell what’ll be the weight loss when lead from scrap batteries are melted?

Regards

Sridhar
e-mail: taraneil123@gmail.com

On February 9, 2016 at 1:23pm
Ganesh wrote:

I am interested.can anybody help me in detailed.l am from Maharashtra.
Mr. Imran l would like to listen from you.so plz give me your no.
And plz tell me when should i call.
Thanks

Ganesh
09822430709

On February 11, 2016 at 5:05am
Saras wrote:

Hi guys,

I want some idea on the salvage value of a used Li-ion battery ( batteries that are expired after electric car usage )

On February 22, 2016 at 4:13am
ABDOU KADER SONKO wrote:

is it possible to get all the informations in french version?
Aniway i am very interesting about batteriesrecycling,i start it already with a netherland friend in my country SENEGAL WEST AFRICA.
THANKS

On February 29, 2016 at 12:46pm
Oneal Lajuwomi wrote:

Dear All,

Our organisation has reached a decision to diversify and enter a new market, which is recycling and manufacturing of lead acid batteries in Nigeria, we are in search of an expert in the sector to help us achieve our dream of a fully functional factory for production of lead acid recycling and manufacturing of batteries.

We will appreciate if you can assist us with a detailed machinery costing of setting up a Small-Medium factory that can produce between 500 -1000 lead acid batteries per/day, installation, commissioning cost, land size requirement and plan of action.

I look forward to hearing from you.

my email is oneal@wavelengthips.com

On March 28, 2016 at 2:10am
Naveed Shaikh wrote:

To introduce ourselves, we are a 30 year Old Company based in Mumbai, India in the field of Lead Oxides, Lead Battery Recycling & Battery Manufacturing .We are manufacturers of these equipment and undertake such Projects on Turnkey basis. Consultancy is also a part of our service. Our Company is a team of Well Experienced technocrats who have experience of more than 35 years Individually.

We have executed projects in Indian Sub Continent, Middle East, Africa, Far East and Russia.

sales@acsleadtech.com
+91-9987077382

On April 7, 2016 at 8:44pm
Debaraj Mishra wrote:

Hi
I have been working LIB recycling for last five years in S Korea
Here recycling has heavy demand.
I would like to start similar in India.
I know the technology but major problem in India is to collect the battery material.
Anybody would join with me in collection process so that I can think about the detail recycling process, starting from manual sorting, mechanical crushing and final product making by hydro process?
Do mail me debraj.mishra@gmail.com.
Thanks

On April 22, 2016 at 2:40am
Lokesh Tripathi wrote:

Dear Sir,

How are you! Glad to know that you want to set up a plant related to recycling, I like to introduce myself as a Manufacturer of special purpose machinery related to recycling and setting up existing plant in more economical manner.
Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market of $33 billion, lead acid (Car Battery) is the most common battery in use.

As per the battery chemistry Lead Acid market value per ton is equal to $1500 which is highly profitable venture to start up also it remains the most suitable battery to recycle; 70% of its weight contains reusable lead.

Now as per my understanding you want to recycle 10 tons of car battery per day right!
We recommend 03 tons of Rotary Furnace with pollution control equipment keeping environment as a necessary aspect.

Whole process will work like this:
Stock of Used Car Battery -> to the battery cutting machine -> desulphurisation of acid from lead -> desulphurised lead sent to furnace -> ingot bullion casted -> sent to refining kettle furnace -> Refined Lead is stacked in Ingot Casting Conveyor.

Our Innovative technology, Design, Precise workmanship, Prompt after sale service has edge to meet demands of today’s industry. The turnkey capabilities allow us to support our client with any types of job from relining Containers to major installations

Should you however need any additional information or clarification in process of finalizing the above 0requirement.  Please call us or write to us.

Mean while thanking you & assuring you best of our services at all the times to come.
We remain…


Your prompt reply shall be highly appreciated.

 

Please contact Me:
Name : Lokesh Tripathi
PH:0091- 9711141615
Location : India , Delhi, (NCR)
Email: info@indotherm.co.in

 

On April 25, 2016 at 10:59pm
Azim khan wrote:

Sir , I m from Karnataka , so I needed ur help to set up a new recycling plant , but her thier is no shortage of batteries , so I want to start new plant

On April 25, 2016 at 11:04pm
Azim khan wrote:

My contact number 9738764268;  9738434739

On April 25, 2016 at 11:08pm
Azim khan wrote:

Email;; azim9750@gmail.com ,

On April 25, 2016 at 11:11pm
Debaraj Mishra wrote:

Is anybody interested for lithium ion battery exporting. We are here in South Korea follows the complete recovery of product from LIB waste battery. We do receive batteries from Japan, US and some other places. If anyone from Europe would be interested to recycle LIB, we would be please do so.
Thanks and regards.

On April 26, 2016 at 1:41pm
Oliver Abara wrote:

Dear Sir, I am into Lead /scrap battery export, I am based in Nigeria and Benin republic. Any interested buyer, individual or company should please contact me. email: oliver12abara@gmail.com

On April 26, 2016 at 11:27pm
Arif Khan wrote:

Dear brothers:
I am Arif from Kabul Afghanistan. i am an engineer with enough experience, I wanted to start a battery recycling company in Kabul but i dont have enough information about battery recycling so i wanted to know about the process, costs and other expenses and if any one wants to take a partner ship.  Please email or you can call me at any time.
Best regards
Email: arif.ahmadzai@gmail.com
Cell #: +93799033111
      +93744889111
Skype: arif.ahmadzai786

On April 28, 2016 at 8:00pm
Natanael Moreno wrote:

I am looking for a company or several companies that can provide me at least 200 metric tons per month of lead-acid batteries. To import them to México.
I want to get in touch with companies in the USA.

Hope you can help.

Email: natanael_moreno@yahoo.com

Cel: +52 1 644 114 6750

On April 30, 2016 at 11:18am
Najiib wrote:

I very happy to this jop, it’s important to us, I am busines man, I have large country without recycling agency. So l want to help our county environment.  And I am ready to this program.

On May 1, 2016 at 1:57am
Aleems wrote:

Send u r mail id & contact number

On May 2, 2016 at 2:14pm
Shaikh waqar wrote:

Sir if i want to buy lithium ion cell scrap or laptop battery scrap what will be the procedure please contact or mail me on my id

On May 3, 2016 at 8:52am
Leeban wrote:

Im from Ethiopia and i have more than 30p ton of battery to export and looking for buyers contact me my email address nebilq@gmail.com

On May 16, 2016 at 9:18pm
Ranthi Dias wrote:

Please let me know if anyone using cleaning chemicals in the battery recycling industry. the cleaning chemical and the application?

On June 8, 2016 at 3:07am
goodness wrote:

Hi Guys, i am very interested in this battery recycling business. Please if there is any information / Knowledge that can make it a success, kindly lay it out. i am very interested.

On June 9, 2016 at 12:21pm
Open Technology Park wrote:

goodness,

Battery recycling business is really hard business.
In EU, US, Canada, Japan and most developing countries you need to be licenced and certified recycling facility to start with recycling.

To recycle batteries you need to develop logistics and build network of battery collection points.

In some countries, used batteries transported in quantities are subject to Environment Protection, Hazardous Materials handling restrictions.

You need need to read carefully your local legislation if you are free to transport 1t of used batteries from City A to your location.

If your stock of used batteries is large and new deliveries pending
you can start with selection, separation and discharging in case of Li-Ion, Li-Po batteries.

It’s still too early to buy technology, chemistry, machinery, equipment, to build recycling facility from the scratch since in EU countries, electric and electronic waste recycling facility collects batteries by itself or gets them delivered as a waste to be disposed of.

So In theory your stock of faulty batteries can grow without any investment.

Buying new Pb car battery you pay extra recycling fee, about $10, so drivers expect to get recycling fee back on disposal of faulty Pb car battery.

To learn more just email me

manta103g@gmail.com
Open Technology Park

On June 17, 2016 at 12:49pm
ron pratt wrote:

take a look at Aqua Metals. 20% owned by Interstate Batteries. The Secondary Lead Recycling alternative to smelting
http://www.aquametals.com/#about

On June 17, 2016 at 1:00pm
Raju Penumatcha wrote:

We are looking for those interested in re-generation of Lead Acid batteries
used as
1) starter batteries ( cars, automotive)
2) traction batteries ( electric vehicles - fork lifts etc.,)
3) stationary batteries ( power supply )

the technology allows re-generation of upto 90 % capacity, and extend the battery life.

re-generation can address :
—Environmentally friendly process
—reduce, re use and re generate

those interested may please contact us for business opportunities.

raju_pvr2006@yahoo.com
Toronto, Canada

On June 30, 2016 at 4:34am
kishan jaiswal wrote:

We have in Kolkata, West Bengal some lithium based batteries to dispose off. Is anyone interested to purchase can mail us to kishan_jaiswal1@yahoo.com immediately.

On July 9, 2016 at 11:24am
Mohd Rashid wrote:

We want to purchase lithium ion battery scrape in tons regularly on cash
parties who can supply the material on competitive price can contact
E-mail;arkrashid20@gmail.com
Mob;9555502324
      8802784136

On July 18, 2016 at 6:08am
Swarock wrote:

We have a huge stock of LIB batteries from electric & hybrid vehicles. Looking for service partners who can collect, transport(with proper packing as per local regulations) and recycle the batteries.
The regions we are looking at are as per priority are:
1. West Europe (Germany, fra, ita, spain, scandinavia, UK)
2. East Europe(Russia & neighbors)
3. China & neighbors
4. USA & Brazil

Licenced and certified recycling service partners only.

Mail me at edspcommerce@gmai.com for further details.

On July 19, 2016 at 4:51am
Chigozie Azunna Ekwuluo wrote:

I the above name and email address, leaved in Nigeria, I have 200 pieces of drained batteries for sell how will I do? In case you’re interested simply reach me through my email or my phone no. 08171902879.

On July 19, 2016 at 10:16am
Leeban wrote:

We have a scrap lead battery more than 2000 ton for sale in Ethiopia we can export to any country

On July 19, 2016 at 1:59pm
Raju Penumatcha wrote:

Hello Leeban,

please contact me at the e-mail address.  we have a business proposal for you.

raju_pvr2006@yahoo.com
best

On July 20, 2016 at 1:48pm
Open Technology Park wrote:

Hello Swarock,

interested in your offer.
Please email me

manta103g@gmail.com
Darius
OpenTechnology Park


Swarock wrote:

We have a huge stock of LIB batteries from electric & hybrid vehicles. Looking for service partners who can collect, transport(with proper packing as per local regulations) and recycle the batteries.
The regions we are looking at are as per priority are:
1. West Europe (Germany, fra, ita, spain, scandinavia, UK)
2. East Europe(Russia & neighbors)
3. China & neighbors
4. USA & Brazil

Licenced and certified recycling service partners only.

Mail me at edspcommerce@gmai.com for further details.

On July 25, 2016 at 5:40am
Khalid Shamsher wrote:

I am interested in setting up a lead-acid battery recycling plant in Pakistan. Finances are arranged already. Need proposals from experts for supply of whole set-up. The objective is to use recovered sulfuric acid for agriculture usage and re-use of lead ingots for battery manufacture.
regards,
Khalid
0092-300-3308918

On July 28, 2016 at 4:08am
Sasi Gopalan wrote:

I am interested in starting a battery recycling unit/new unit. Can somebody help me with technical details, where to buy machinery etc.

On July 29, 2016 at 5:25pm
Raju Penumatcha wrote:

Hello Sasi Gopalan,

please contact us at the e-mail address.  we have a business proposal for re-generation of Lead Acid Battery.

best

e-mail:  raju_pvr2006@yahoo.com

On August 6, 2016 at 2:51am
A K wrote:

Hi All,
I want to setup a modern Lead Acid Battery Recycling plant in Nigeria, anybody can enlighten me about availability of Lead Acid battery scrap and feasibility and survival of this industry in terms of Nigerian economy and present situations.
Proposed capacity is 100MT/day.

On August 8, 2016 at 1:35pm
Raju Penumatcha wrote:

Hello A K,


we offer technology and training support,  for Re-generation of Lead Acid Battery.

—curative re-generation would allow extending the life of a used ( end-of-life)  lead acid battery by an additional 100%
—preventive maintenance would allow in-use lead acid battery by an additional 100 to 150%, and also reduce the energy used for charging, over the use of the battery life.

we are interested to offer the idustrially proven technology and training is available.
best
e-mail:  raju_pvr2006@yahoo.com

On August 11, 2016 at 10:44am
jas wrote:

Hi! there, I want to setup a lead acid battery recycling plant in India for a capacity of 10MT / daily. I want start with small unit first. please can anybody help me with building up of plant. Preferably I like to setup this in Uttar Pradesh, India

On August 12, 2016 at 11:00pm
Naveed Shaikh wrote:

Dear,

Anybody with availability of Lead Acid Battery Scrap please let us know by email.

To introduce ourselves, we are a 30 year Old Company based in Mumbai, India in the field of Lead Oxides, Lead Battery Recycling & Battery Manufacturing .We are manufacturers of these equipment and undertake such Projects on Turnkey basis. Consultancy is also a part of our service. Our Company is a team of Well Experienced technocrats who have experience of more than 35 years Individually.
We have executed projects in Indian Sub Continent, Middle East, Africa, Far East and Russia. We have 70 projects to our credit.

sales@acsleadtech.com
+91-9987077382

On August 14, 2016 at 10:13am
Gibson John wrote:

Hello everyone I m looking for a serious partner I can sign a contract with because I have about 30 tons of drean lead acid scrap battery in stock already and I can export to any country only serious buyers should contact me please and I will show you our goods that is already in stock by picture through email thanks

Email giggslan80@Yahoo.com or giggslan80@Gmail.com
Or u can reach me on phone +23408181039941 .
Best regards
Gibson John

On August 26, 2016 at 7:55am
muhammad iqbal wrote:

‘‘consumption ,preparation ,import and recycling of batteries in Pakistan.’‘

On August 29, 2016 at 8:03am
pawan mundra wrote:

I want to set up Lead Acid Battery Recycling Plant.

On August 29, 2016 at 1:22pm
Raju Penumatcha wrote:

Hello Pawan Mundra,

we can propose a business model for Lead Acid Battery re-generation, with capital requirement far below that of re-cycling.

re-generation allows, pollution free, profitable Lead Acid Battery business.

let us know your interest.

raju_pvr2006@yahoo.com

Raju

On August 31, 2016 at 2:32pm
Leonard Dugan wrote:

Hello, Looking for a company in the Dallas / Ft Worth area that buys li-ion, NiCad, NiMH, batteries. I have batteries and cells from home use, medical equipment, laptops, drills, etc. please email me or post the information here. I have around 500 pounds total to sell.
Thanks Leonard

On September 9, 2016 at 8:54pm
Amol Jadhav,Pune wrote:

We have designed a technology where no need to replace the old battery.Its environment eco friendly cost saving project to all Battery users.Pls revert if interested on +917066667883.We can start business any where in India.

On September 21, 2016 at 3:07am
leila wrote:

Hello
Iam studying master chemistry engineering.my project is Recycling Of Valuable Metals From Nickel Cadmium Waste Batteries.I will do my tests other weeks but I have some problem about process if you can help me please guide me.thanks
Email:z.khamooshi@gmail.com

On September 23, 2016 at 7:33am
leila wrote:

Hello
I want to set up Ni Cd waste batteries recycling plant.please can anybody help me with information especially Pyrometallurgical method to recycling battery.
Thanks
Email:z.khamooshi@gmail.com

On September 28, 2016 at 1:44am
Rahul wrote:

hello
Can we get in anybody india scrap seller /buyer contact-8103095763

On October 22, 2016 at 8:36pm
Lubna Hanif wrote:

I am based in California USA and I am desperately looking for Car battery recycling plant.
If anybody can help me with information. I will be really grateful.

On October 24, 2016 at 10:39pm
JS Kim wrote:

I am looking for companies who requires ‘battery recycling’
Our company(south korea) is very qualified and well experienced in field. We already doing buisness with recycling batteries in china, India, Turkey and South Africa. We can do all kinds of batteries in any term.
Pls contact me If you interested;

Jiseonkim0807@gmail.com
+91 9618098812 ( india )
+82 10 3906 6445 (Korea )

On October 25, 2016 at 11:08pm
Lubna Hanif wrote:

Looking for used car lead battery recycling plant. Any information will be greatly appreciated.
lubnahanif583@gmail.com

On October 26, 2016 at 2:30pm
Haider wrote:

How can one obtain a license to produce green lead

On October 27, 2016 at 12:03am
Imran khan wrote:

Hello,

I saw many of them looking for used battery recycling plant . Please contact Aleem khan +919341836119 or +918123561118 . We are planning to sale our battery recycling plant located in India with all pollution control board of India certificate plant full loaded running plant with all machineries and equipments along with land .all certificates are updated and valid.serious person who is looking for battery recycling plant buyer can contact us.

Thanks,
Imran khan
8123561118

Sent from my iPhone

On October 30, 2016 at 12:40am
Fahad wrote:

I want to setup a modern Lead Acid Battery Recycling plant in Pakistan , anybody can enlighten me about availability of Lead Acid battery scrap and feasibility and survival of this industry Thankyou waiting
For reply
Email sales@faithmetal.com.pk

On November 4, 2016 at 5:15pm
Christian wrote:

Hello

I am WEEE recycler based in Lagos state of Nigeria. i have large lithium stock of scrap batteries and have the capacity to increase depending on Mou with a buyer. $1.12/lbs

I seek buyers.  kindly email cademicsgroup@gmail.com

Christian
+2347012733347

On November 6, 2016 at 5:55am
Sandeep wrote:

I want start smelting battery lead scrap in electric machine what’s the process and how much time 50 kg battery lead scrap melting process and 50 kg battery scrap after melt not plastic only lead scrap how much quantity or kg after smelt I receive solid lead in 50 kg

On November 16, 2016 at 12:12am
okoso wrote:

I am based in Mongolia and want to setup a Lead Acid Battery Recycling Business. Any information will be greatly appreciated.

Thank you
okoso13@yahoo.com

On November 16, 2016 at 1:03pm
Wald wrote:

Dear Sirs.

I have a great amount of scrap batteries monthly to recycle in Paraguay South America.

If there is any company with logistics to pick up the batteries are very welcome.

Please send a list of price for my email with the prices that you pay for each type of battery by Ton.

Thanks..Wald..Whatsapp +595983132181

On December 2, 2016 at 8:14am
farsad wrote:

We supply lead acid scrap. Any interested buyer should please email to get details.

On December 2, 2016 at 12:54pm
farsad wrote:

I look forward to hearing from you. Email :infoelcatek@gmail.com

On December 11, 2016 at 4:30pm
paul wrote:

have large regular amount of phone batteries for recycling serious inquiries please

On December 13, 2016 at 11:20am
Balaji wrote:

Hi all, We are leading suppliers of lead acid battery scraps in Tamil Nadu, India established in the year 1997. We can supply minimum of 150MT per month. Kindly contact us by phone +91-96262-52520 or email to balaji@electroindia.net

We are interested to buy battery scraps from other countries. Necessary import certificates are available. Kindly contact us to discuss further.

Regards,
Balaji
+91-96262-52520
balaji@electroindia.net

On December 14, 2016 at 11:23am
CrossBar wrote:

Hi, Im looking for a company that would recycle/dispose large quantities of Lithium Polymer batteries, coming from e-cigs for 70-80K month. Could you point me in the right direction?
THANK YOU
Beth Barton

On December 27, 2016 at 9:43pm
Malyasee wrote:

I am an expert in setting ups a” Lead Acid Battery Recycling Plant” with less capital cost,any one interested do let me know,

Thanks

On January 9, 2017 at 8:49am
Tarun wrote:

Hi,

I am in battery field for around 12 years. I have battery business (start-up) in North India. I have well established market (dealers/distributors).

Is any person interested to invest in my business? Also, I am looking for manufacturers, who can provide me automotive/inverter batteries.

Thanks

On January 17, 2017 at 8:38am
Debaraj Mishra wrote:

Hi
My South Korean company would like to start lithium ion battery recycling unit in India soon. We would like to contact as many as suppliers who can supply waste LIB batteries. Is there anybody who would supply such materials to us regularly?
Thanks. mail me debraj.mishra@gmail.com

On January 23, 2017 at 12:04am
Dr. Venu Katta wrote:

Hello Everyone, Firstly, I would like to introduce myself, I am Dr. Venu Katta, x Director & VP for Exide Technologies Canada. I always had a dream to start a Lead Acid Battery Manufacturing Plant in India. I lived here in Canada for past 20 Years, recently I moved to India to start the Lead Acid Battery Manufacturing Plant in south part of India. I then procured Land and Constructed the Unit with North American Standards. I have all the Licenses which includes Red Category Pollution License and Small Scale Industry License and all other Industrial Licenses in place issued by the Pondicherry Government. Due to unforeseen reason, i have to move back to Canada again. If anyone is interested to take over the project along with the land and building with HT approved electricity in place. I am ready to sell the property and or if someone is interested to lease the property i am willing to give away the Mobile entire established project. Please contact me for further details either via phone or email. My contact information is Mobile Number 001-905-531-2551 and email id: v.katta@hotmail.com.
I thank you all for your kind cooperation and appreciate your support and help in advance!

With Best Regards,
Dr. Venu Katta

On January 31, 2017 at 5:19am
pawandeep singh wrote:

hi Beth,
kindly share your contact details. we can help you.
thanks

CrossBar wrote:
Hi, Im looking for a company that would recycle/dispose large quantities of Lithium Polymer batteries, coming from e-cigs for 70-80K month. Could you point me in the right direction?
THANK YOU
Beth Barton

On February 7, 2017 at 12:38am
Abraham wrote:

I am impressed with this business as it offers great opportunity. I visited a Battery Recycling plant some months ago and I love to start up same with aid of foreign partners.

Anyone with detailed plan of this business, should reach me via the email. holuafolayan@gmail.com

On February 8, 2017 at 11:41pm
Lokesh Tripathi wrote:

Dear Sir,
How are you! Glad to know that you want to set up a plant related to recycling, I like to introduce myself as a Manufacturer of special purpose machinery related to recycling and setting up existing plant in more economical manner.
Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market of $33 billion, lead acid (Car Battery) is the most common battery in use.
As per the battery chemistry Lead Acid market value per ton is equal to $1500 which is highly profitable venture to start up also it remains the most suitable battery to recycle; 70% of its weight contains reusable lead.
Now as per my understanding you want to recycle 10 tons of car battery per day right!
We recommend 03 tons of Rotary Furnace with pollution control equipment keeping environment as a necessary aspect.
Whole process will work like this:
Stock of Used Car Battery -> to the battery cutting machine -> desulphurisation of acid from lead -> desulphurised lead sent to furnace -> ingot bullion casted -> sent to refining kettle furnace -> Refined Lead is stacked in Ingot Casting Conveyor.
Our Innovative technology, Design, Precise workmanship, Prompt after sale service has edge to meet demands of today’s industry. The turnkey capabilities allow us to support our client with any types of job from relining Containers to major installations
Should you however need any additional information or clarification in process of finalizing the above 0requirement.  Please call us or write to us.
Mean while thanking you & assuring you best of our services at all the times to come.
We remain…

Your prompt reply shall be highly appreciated.

Please contact Me:
Name : Lokesh Tripathi
PH:0091- 9711141615
Location : India , Delhi, (NCR)
Email: info@indotherm.co.in

On March 3, 2017 at 3:13pm
anita wrote:

Hello
have you been search for scrap metals , you have found the right place were you can get your urgent scrap metal. search no further, We sells Scrap metal recycling and scrap metal yard, We also Sell recycle metals of all types, shapes and sizes. Our metal scrap yard is equipped to handle small loads of household metal scrap and large loads of commercial scrap metal salvage. We sell metals at the lowest prices and have a reputation in the Valley of the Sun as being fair, honest and professional.EMAIL: clintonmathewscrapmetalcompany@gmail.com whatsapp or call +2347059186258

On March 28, 2017 at 12:32am
Sohan wrote:

Hello
      We are lead acid batteries manufacturer and recycler in India (Rajasthan). We have been in this business from last 10 years. If any one like to start this business in India we can help in all feel free to contact. We would also like to establish lead acid recycling plant outside India as well.

Thanks

sohanchouhan3@gmail.com
+919784289007 (WhatsApp)
skype:sohan2479

On April 19, 2017 at 5:13am
Mansoor wrote:

I want to start battery/battery recycle business in Afghanistan, the opportunity is very good for such business in here, the demand is very high here,

All I want is to have an expert to guide me trough the start of business or guide me to have
essential machinery for this purpose.

Anyone who want to help me please reach me with email below;

mansooraziz16@gmail.com

On May 18, 2017 at 9:17pm
Subrata pal wrote:

I want to start battery recycling business in India , in India state of Tripura . Essential machinery for this purpose…

On May 20, 2017 at 12:46am
Naveed Shaikh wrote:

Dear Mr. Subrata Pal,

Please contact us @ 91-9987077382

On May 30, 2017 at 8:13am
yerry easy wrote:

Write us today on yerryeasy@hotmail.com, we can be your agent/representative. Also we can help you with recycling services.

On June 13, 2017 at 10:33am
Nazmul Hasan wrote:

Hello
This is Nazmul Hasan from Bangladesh.I need a small lead Battery recycling plant
10ton daily waste scrap ,dross
My finished goods will b hard lead/raw lead
Low investment

XENCELL Battery
Ranabola,Taslima plaza
Turag-Dhaka-1230

On June 13, 2017 at 10:53pm
Imran Khan wrote:

Hello,
Nazmul hasan.
Please contact me my factory is for sale in India, also share your contact
Contact or Watsup
919341836119

On June 16, 2017 at 12:48pm
Md Shariful Islam wrote:

Hello,
I’m from Khulna,Bangladesh.  I’m a student. Beside my study I run a small business on lead battery recycling. I collect scrape battery from many districs . I just buy scrape batteries which are used in bus, truck, car, auto,  motor bike, ips, solar, cng, telecommunications tower, touch light batteries and so on. From recycling this I come out pure lead and sell to my nearby company. But at now I want to export lead to foreign countries.  If any one want to buy lead from me please contact with me via email.

My email :- mdsharifulislam.msis@gmail.com

On July 4, 2017 at 10:05am
Sridhar wrote:

Hi all

This is sridhar from Chennai

Am very much interested in this business but I don’t have any idea about this.  Am looking for the investor to start this business.  I can arrange land and all licence to start this business.  If any one interested to expand your business at Chennai please contact me at

Sridhar 919543342667

On July 4, 2017 at 1:16pm
american manganese wrote:

http://americanmanganeseinc.com/

American Manganese Inc. is a Critical Metal Company Focusing on Recycling Lithium Ion Electric Vehicle Batteries.

there you go!

On July 6, 2017 at 9:52am
american manganese wrote:

AMERICAN MANGANESE INC. REPORTS WORKING RECHARGEABLE BATTERIES PRODUCED FROM RECYCLED NMC CATHODE MATERIALS

Kemetco Research Inc. has successfully produced lithium:nickel:manganese:cobalt (Li:Ni:Mn:Co) (NMC) cathode material and working coin cell rechargeable NMC batteries using recycled lithium, nickel, manganese and cobalt from American Manganese Inc.‘s patent-pending lithium-ion battery cathode material recycling process.

Preliminary battery cycling test of the NMC battery has demonstrated that it reached the targeted battery capacity, which further proves American Manganese’s patent-pending battery recycling process can recycle and refabricate the NMC material to make new NMC batteries.

“Based on these preliminary results,” said Norm Chow, president of Kemetco, “it can be speculated that the American Manganese upcycling technology represents the world’s first NMC battery produced from AMI’S closed loop recycling process.”

“These results continue to validate the AMI process,” said Larry Reaugh. “With this phase of test work, we’ve taken very complex lithium-ion battery cathode material from the recovered components through the reconstitution of the NMC cathode materials to produce working chargeable cells.”

Battery fabrication and assembly

Recycled NMC was generated by precipitating the metal components from a leached solution of commercially available feedstock. XRD (X-ray diffraction) of the reconstituted NMC material has characterized the material as having a perfect ratio of Li:Ni:Mn:Co—1.06:0.33:0.33:0.33—a 100-per-cent match to the commercial battery grade of NMC.

This cathode material mixture was subsequently coated onto aluminum foil and dried for two hours at 120 C in a vacuum oven to form the lithium-ion battery cathode.

The button cell batteries were assembled as follows: top cell case, cathode, separator, anode, spacer, ring-shaped spring and bottom cell case. The anode was made from purchased graphite. The ring-shaped spring was placed between the negative casing and the spacer to ensure adequate pressure was applied to the cell components. Both the spring and the spacer are made from stainless steel. A thin layer of polyolefin was used as the separator.

About American Manganese Inc.

American Manganese is a diversified specialty and critical metal company focused on capitalizing on its patented intellectual property through low-cost production or recovery of electrolytic manganese products throughout the world, and recycling of spent electric vehicle lithium-ion rechargeable batteries.

Interest in the company’s patented process has adjusted the focus of American Manganese toward the examination of applying its patented technology for other purposes and materials. American Manganese aims to capitalize on its patented technology and proprietary know-how to become and industry leader in the recycling of spent electric vehicle lithium-ion batteries having cathode chemistries such as: lithium-cobalt, lithium-cobalt-nickel-manganese and lithium-manganese (Please see the company’s Jan. 19, 2017, press release for further details).

On July 7, 2017 at 4:26am
darius wrote:

Hi,
could you kindly explain, why emailed submissions from this page get delivered
as unformatted ASCII text email, making hard to read them ?

Ok, I know an old End Of Line / New Line formatting problem in Linux vs. MS Windows
problem, already solved 20 years ago.

Could you upgrade serveer settings to deliver formatted submissions via e-mail ?

Already recycled 10,000+ Li-Ion used batteries, giving them second life.

thank you
darius

On July 15, 2017 at 5:21am
RAJAT ANAND wrote:

Hi,

We at Mettherm, provide complete turnkey solution for Battery Recycling for extraction of this lead in usable form. We provide Battery Recycling Plants, Lead Ore Smelting Plants, Lead Refining Plants, Battery Breaking and segregation plant and consultancy till trial production.

You can visit our website mettherm.com for more details and can also request for a quote depending on the capacity of the plant required.

We are based in Faridabad, New Delhi NCR, Haryana

Thank you,

Rajat Anand

On August 6, 2017 at 9:57am
Sulaiman Meghjani wrote:

We are Toronto and UK - Hounslow based looking for opportunity into battery recycling.

We can be your reliable partners in Collection, managing stocks etc at these locations. If any body is interested in sharing revenues, please contact us info at grinva . com

sulaimanmeghjani at yahoo . com

On August 14, 2017 at 9:26pm
Optimum Battery wrote:

We are a Saskatoon based business that sells used/refurbished automotive batteries and provides battery collection/drop-off services to the surrounding area.

We try to Reduce, Reuse, and Recycle - therefore, each battery we collect is tested, and if possible refurbished for resale before it is eventually recycled. 

If you are an individual or business in need of a solution to your constant scrap battery accumulation, please don’t hesitate to contact us!

Check out our website at www.optimumbattery.ca

On September 18, 2017 at 4:44am
Kristina Malgina wrote:

We are a trading company in Hong Kong.
Currently one of my clients is looking to buy a large amount of used lead-acid batteries (500-5,000 tons per month) to be shipped to our port.
We do not have a preference on the exporting country, as long as the supplier is reliable and cost-effective. However, I do not have experience with lead-acid batteries specifically and am struggling to find suitable candidates for such exports.

If you are an individual who has information regarding where I can find such exporters, please do reach out - any information would be helpful.
If you are company that is able to fulfill such requirements or are looking for a buyer, please do get in contact with me via email- I would be very happy to hear from you.

Thanks in advance!
kristina.malgin@gmail.com

On September 22, 2017 at 11:09pm
Mohammed wrote:

I am looking to start recycle of scarp batteries I would like to know more about the field of recycling and demand in the market. My contact number mentioned below
Thanks
Mohammed
00917010317274

On October 13, 2017 at 3:59am
abdul moiz wrote:

we have large number of silver oxide button cells .we are looking for some buyers for these kind of batteries .
kindly contact on
00971558789898.

On November 1, 2017 at 1:09pm
MOHD RASHID wrote:

Require in bulk quantity spent mobile Lithium ion
batteries for Recycling.
Please contact; 91-7550633477
e-mail; arkrashid20@gmail.com

On November 1, 2017 at 11:05pm
haiytham wrote:

interested pl. contact me

On November 6, 2017 at 2:48am
samer wrote:

hey dear ;

we have monthly 300 mobile phone batteries we love to know prices about it and if u have free shipping…..

thank you, waiting your request.

On November 16, 2017 at 9:54pm
Rob wrote:

Hi,

Anyone here working in a Hydrometallurgical process of battery recycling?

Also, is anyone here doing research on rare earth metals in battery waste?

Thank you for anyone who can help connect me with people involved in this.

my email: salamat-r@organo.co.jp

On December 18, 2017 at 8:26am
Walter Esteves Incio wrote:

Experto en Reciclaje de baterias plomo acido, PP plastico de cajas, soluciones acidas, Plomo Bullion, Plomo refinado 99.99 %, plantasde oxido de plomo.  Diseño - Fabricacion en cualquier escenario, baterias industriales, etc., mi ciorreo electronico es:  esteveswalter1@gmail.com

Tesis de grado en topicos de reciclaje

On December 18, 2017 at 10:49am
Walter Esteves Incio wrote:

Excelente informacion,  soy experto en reciclaje de baterias, experiencia maa de 30 años Plomo bulion, refinado al 99.99 %, plastico, soluciones acidas etc mi correo es:
esteveswalter1@gmail.com

On December 25, 2017 at 9:40am
Saeed Ur Rehman wrote:

Hi All,
I am Saeed from Jeddah Saudi Arab and I have a Lead refining factory and I want to start my business in Pakistan anyone who can help me in this regards can contact me as I have some queries about this factory also about the remaining material after recycling the lead from batteries I need any research center any were in the world you can easily contact me on my Whatsapp, IMO, FB NO 00966580002834,00923129890459 or Saeedlucky@icloud.com

On December 31, 2017 at 6:39am
Junaid wrote:

I am intrestes in this business scrap and battery recycle. I am from india if anybody intersted   Contact me +919015367919…. syedmashkoor4@gmail.com

On January 2, 2018 at 8:57am
Maureen Onwuka wrote:

SUPPLYING USED BATTERIES
Hello, i recently got into the supply of used inverta battery when i was contacted to supply a certain quantity here in Nigeria, West Africa by an Organization that was exporting same to Europe in 2016. I have been doing research on the market for battery recycling and i know the business to be lucrative though tedious. Now am interested in this business but mostly in the supply of the Starter battery (Cars, Automobile), Traction (Electric Car) or Stationary battery (Power Supply).
Please anyone that is interested to get them from Nigeria should contact me.  Nigeria is a veritable ground for this business due to the high usage of batteries because of power shortages and the need for alternative sources as well as the population of car users which is quite high. 
Kindly respond.

Regards,
Maureen Onwuka
nikky2002ng@gmail.com

On January 4, 2018 at 11:30pm
Trang wrote:

Dear Sir/Madam
NEED TO BUY A BIG QUANTITY OF UNUSED LITHIUM BATTERY FROM JAPAN/INDIA.

My name is Trang. I am a marketing manager of ANHUA TAISEN RECYCLING COMPANY. .Our business is recycling dispose lithium battery (18650 batteries) in our factory in China including:  cell phone battery, laptop battery, electronic car, industrial railway battery, aviation battery….

we need to buy/ import a huge of dispose/unused lithium battery in Japan/India with whatever status of battery.  We are looking for the source of unused lithium battery to buy, if you have or you know some kinds of unused lithium Battery Company/ manufactures/seller in Japan/India who wants to sell, please introduce to me.
Look forward to getting your news.
Best regard

My email: trang-marketing@tai-sen.cn

On January 9, 2018 at 6:46am
David A wrote:

Dear Sir/Madam,
I have 1,000 pcs of VRLA Batteries (12v, 150ah)  for Recycling or Regeneration in Rwanda(EA) and seeking ideas & partners to do this in the shortest time possible.

Similar opportunities apply for othe East African countries (Uganda,Ke,TZ, Juba)

Please advise on
kenninvest@gmail.com

On January 9, 2018 at 5:31pm
darius wrote:

Hi David,
Hi Allan,

I have already emailed you

you have some options open.
In Europe VRLA Pb batteries are collected for free by recycling plant or its agents,
or you can negotiate a price per kg, as a source of Pb metal.

Other option is to diagnose every battery and use fast charger to get some back to life and
sell as used VRLA batteries at half price.

If you know what are the sources of used VRLA ( large or small UPS system, security system, medical equipment , personal use)
I can tell you more.

Just list me Amperage (Ah), Voltage (V), size, type, manufacture year by manufacturer.

Since East Africa lives close to China, local market prices of new or refurbished VRLA batteries may be much lower vs. Europe.

I am interested to import your VRLA 150Ah batteries to Europe for some refurbishing-recycling procedure

Darius

Open Technology Park
manta103g@gmail.com

BTW ,
just attach some images

On January 22, 2018 at 1:10am
dinesh wrote:

Hi, I m looking to set up a Lithium ion base battery recycling plant with most efficient way to extract lithium and other metal. kindly guide me that which companies are offering help to set up in India

On January 22, 2018 at 6:48pm
darius wrote:

Hello Dinesh,

I am not sure about profitability of Li-Ion battery recycling plant, since you need to apply for public funding, subsidy first.

I am interested to buy largest Li-Po Li-Ion batteries by size, weight and current (Ah) and offer regeneration, preselection technology since it makes sense to refurbish and give second life to such expensive electric hybrid car or bus Li-Ion batteries.

Just purchased 85 90Ah Li-Ion from electric car and started regeneration process.

Many may claim it doesn’t make sense. Exactly, but I already succeeded to regenerate Pb car batteries, gel batteries and what comes next are exactly Li-Ion heavy current, amperage batteries since the price of new ones is great challenge.

I am going to buy Toyota Prius electric and hybrid battery packs for regeneration.

Since Li-Po, Li-Ion battery transportation restrictions apply, I am not going to import large quentities of Li-Ion large current batteries from one continent to another to meet all safety regulations and cut the costs.

I would like to establish a network of Li-Lion batteries world-wide and deliver technology solutions, professional chargers and general guidance.

10 years ago I regenerated large quantities of Li-Po Li-Ion cell phone batteries with great success due to limited availability at local markets.

Let me know your opinion and your interest

Darius Jack
Open Technology Park
manta103g@gmail.com

On February 1, 2018 at 7:40pm
Andy Jung wrote:

Dear All

We are recovering valuable metals from LIB in south Korea. I am looking for LCO or/and NCM powder from the used LIB. Please contact me if you can supply such powder materials.

Thank you.
Andy Jung
chemtex.jung@gmail.com

On February 19, 2018 at 1:15am
viswanadh wrote:

Hi,i’m planning to start battery scrap dealer in andhra pradesh india. my question is what are the license required to start this…

Please help me.

On February 22, 2018 at 1:04am
mr john kojo wrote:

i sell lithium’s batteries in tons if you have interest of buying from me. you can contact me on my email or whatspp. email: johnkojomarketing@gmail.com. whatsapp number is +233552263100

On February 23, 2018 at 11:39pm
fiona wrote:

looking for lead acid battery from world .  if you know where to get,how to get ,who can supply, pls let me know here

best regards
fiona
wechat:+0086-15356118280
oopscolor @ 163 . com

On February 25, 2018 at 10:40am
mr john kojo wrote:

i have lithium battrties and acid battries used for sell in tons

On February 25, 2018 at 11:00am
mr john kojo wrote:

Hello,
I’m from ghana.  I’m a business mant. Beside my study I run a small business on lead battery recycling. I collect scrape battery from many districs . I just buy scrape batteries which are used in bus, truck, car, auto,  motor bike, ips, solar, cng, telecommunications tower, touch light batteries and so on. From recycling this I come out pure lead and sell to my nearby company. But at now I want to export lead to foreign countries.  If any one want to buy lead from me please contact with me via email.

My email :- mdsharifulislam.msis@gmail.com

On February 25, 2018 at 11:08am
mr emeka wrote:

Hello,
  I’m a Business man. Beside my study I run a big business on lead battery recycling. I collect scrape battery from many districs . I just buy scrape batteries which are used in bus, truck, car, auto,  motor bike, ips, solar, cng, telecommunications tower, touch light batteries and so on. From recycling this I come out pure lead and sell to my nearby company. But at now I want to export lead to foreign countries.  If any one want to buy lead from me please contact with me via email.
also sell lithiums batteris

My email :- emekabattries@gmail.com

On March 6, 2018 at 4:55am
Simone wrote:

Hello,

we have lot of used li-ion batteries from Ev and e- bikes, most of them still have capacity.
Anyone interested into buy them?

On March 6, 2018 at 3:38pm
darius wrote:

Hi Simone,
interested in your li-ion batteries from Ev and e-bikes.

Let me know your geolocation and attach some images of your stock

darius
Open Technology Park
manta103g@gmail.com

On March 9, 2018 at 12:53pm
darius wrote:

Hi Simone,

since I don’t get reply from you and gmail.com is no more reliable today, not supporting re: re: re:

Please email me at

jack.investigator@yandex.com
Open Technology Park

This is my email sent to you, not replied yet.


Thank you Simone for your kind reply.

First image: 90Ah Li cells by Headway (f. Winston), installed some years by a company from Italy, converting Fiat Doblo to all electric.

I am interested. The problem is these Li cells simply swell ( pillow effect), not fit for EV since can broke apart any closed apartment for batteries ( 74 in series).
I have a number of them under my table, completely discharged ( nominal voltage is 3.2V , today 0.2V)

Images 2 and 4
e-bike packs, really inrterested in, since I build intelligent Li-Ion spot welders and use old Li-Ion cells for tests.

Image 3 Li-Po cells and packs, swell badly, should be recycled as soon as possible since can get a fire at random.

I recentl;y purchased Li-Po power bank (new), which burnt out at the shop, still in original box, so I was not aware of.

Image 5 - old Ni-H cells from e- tools, old technology, no use , I recycle them.

Please let me what number of 90Ah cells by Winston
and what number of e-bike battery packs ( BMS, balancer module removed)
can be collected and what are your terms.

I am looking for modern battery packs for Tesla, Toyota Hybrid and other EVs

best regards,

Darius

On March 17, 2018 at 9:12am
Hakim wrote:

Hello
plz email me if you you want to buy recyclable car batteries
hakeem_esdeen@hotmail.com

On March 17, 2018 at 10:05am
Trang wrote:

Dear Dinesh
Could you contact to me in email

My company has plant to set up factory in other countries once these countries has enough capacity of lithium battery scrap to run (at least 600 tons month).
Could you tell me about the potential there
skype   cupi2013

On March 18, 2018 at 6:34pm
Trang wrote:

Dear Simone
Can you share your stock information? We would like to buy a big volume of lithium battery with comparetitive price
Best regard

email: dianaross.smith@gmail.com

On March 20, 2018 at 5:47pm
Open Technology Park wrote:

My Dear Friends,

to match used batteries buy/sell offers we need on-line transaction exchange system, known from solar panels market.

To make things short, just make your offer real, give your buy/sell price,
give your geolocation to let us calculate pick-up or delivery costs / courier + your price to make trade offer profitable for both parties.


Please be aware, email by gmail is not supporting business talks, since your reply can always be sent to trash or spam box and it takes a lot of time to track thread.

Linkedin or Twitter are real-time chat services, so you can talk and get immediate response and make business on-line.

If you know how can I get and buy 100 used Li car batteries per month or a stock of 1,000 in Europe, please let me know, since I don’t love the idea every used Li car battery should be recycled.

I have already given second life to hundreds of Li, Pb used batteries and it makes sense.

This month I start tests with garage production of gel batteries since sulphur acid new or used car batteries are of limited use off-grid renewable energy systems due to risk of acid leakage

Let me know if you can use Twitter

best regards,

Open Technology Park
Open Fabrication Lab
Darius Jack
jack.investigator@yandex.com

Twitter:
jack.investigator@yandex.com

Twitter support personal messages and notifications
and images can be easily attached, as well as web links

On March 30, 2018 at 10:55pm
Kashif Tai wrote:

Hi All,

I am looking for Lead Powder /Paste in big quantity every month.
If anybody can offer me, please let me know soon.

Regards

Kashif
Marium.ent@hotmail.com
00923219210739

On April 8, 2018 at 8:42pm
Cardano Li wrote:

This is Cardano.Our company wants to buy dispose/waste/scrap lithium battery as much as possbile. Our company capacity is 10,000 tons/month, so we try to collect worldwide.
For price, it depends on the kind of waste lithium battery, when we have picture, we can estimate the price.
From you, if you collect enough 20 tons for one container, we can buy immediately and export to China.We now need to purchase recycled products:  I: Finished products: scrapped laptop battery, scrapped battery, scrapped cell phone battery, scrapped electric vehicle battery
II: Material:Cathode film scrap (lithium cobalt),Cathode film scrap (Ternary Lithium battery),Battery core scrap (Lithium cobalt without liquid) ,Battery core scrap (Ternary Lithium battery without liquid),Battery liquid core scrap (Lithium Cobalt),Battery liquid core scrap (Ternary Lithium battery) ,Cathode powder scrap,Cathode slurry scrap (Lithium Cobalt),Anode film scrap,Cathode slurry scrap (Ternary Lithium battery)。
I send to you my skype: cardano.lee, please accept and then we can discuss easier.
our factory 10 years focusing on reproceeding waste Li-ion battery with environment friendly way and advanced high technical method.Is
t possible to take chance for cooperating with your company based on mutrual benefits?
Hope to hear from you soon with my sincere appreication.
Thank you and Best regards

Ms Cardano Li   (wechat / what’App : +86 18503066565 )
Global Purchasing Director
Skype:cardano.lee
Email:purchaser@recycling.org.cn

On April 11, 2018 at 3:57pm
Fatima Susana Martinez Lopez wrote:

To whom this might concern,

Hello, my name is Fatima Susana Martinez Lopez. I am currently an honors student at Wake Technical Community College in the state of North Carolina. I have been working on a research project about batteries and I noticed that many people that attend my college campus do not know how to properly dispose of their old batteries. Currently, there is not a specific battery recycling program. While working on my research project my honors advisor and I were discussing how to initiate a battery recycling program on our campus. So, I came across your website and I am impressed at how well organized you are about recycling batteries. By any chance, could you give us some advice from your experience on how to implement a Battery recycling program like yours on my college campus?

We are mainly interested in the logistics of how to properly collect the used batteries but any advice would be greatly appreciated.

Sincerely,

Fatima Susana Martinez Lopez

On April 12, 2018 at 12:59pm
Imran Khan wrote:

Hello Suzan,

Please watsup me@ +918123561118 for the information related to recycling.
Thanks
Imran

On April 22, 2018 at 2:44am
Ghazi wrote:

Hi all,
i want to open plant recycling of batteries in Saudi Arabia i need your help plz as i dont have any information abouy the best company to buy the equipment

On April 23, 2018 at 10:59pm
Lokesh Tripathi wrote:

Dear Sir,

How are you! Glad to know that you want to set up a plant related to recycling, I like to introduce myself as a Manufacturer of special purpose machinery related to recycling and setting up existing plant in more economical manner.
Batteries are expensive and have a relatively short life span. As discarded batteries grow by the tonnage, entrepreneurs are enticed to start a business in recycling. With an annual world market of $33 billion, lead acid (Car Battery) is the most common battery in use.

As per the battery chemistry Lead Acid market value per ton is equal to $1500 which is highly profitable venture to start up also it remains the most suitable battery to recycle; 70% of its weight contains reusable lead.

Now as per my understanding you want to recycle 10 tons of car battery per day right!
We recommend 03 tons of Rotary Furnace with pollution control equipment keeping environment as a necessary aspect.

Whole process will work like this:
Stock of Used Car Battery -> to the battery cutting machine -> desulphurisation of acid from lead -> desulphurised lead sent to furnace -> ingot bullion casted -> sent to refining kettle furnace -> Refined Lead is stacked in Ingot Casting Conveyor.

Our Innovative technology, Design, Precise workmanship, Prompt after sale service has edge to meet demands of today’s industry. The turnkey capabilities allow us to support our client with any types of job from relining Containers to major installations

Should you however need any additional information or clarification in process of finalizing the above 0requirement.  Please call us or write to us.

Mean while thanking you & assuring you best of our services at all the times to come.
We remain…


Your prompt reply shall be highly appreciated.

Please contact Me:
Name : Lokesh Tripathi
PH:0091- 9711141615
Location : India , Delhi, (NCR)
Email: info@indotherm.co.in

On April 30, 2018 at 11:09pm
Abdul Akinpelu wrote:

I will like to have use battery recycling factory and where to get the machine

On May 1, 2018 at 9:19am
Riyas wrote:

Hi
I wish to import scrap batteries to India if you have any idea about this please give me the information

On May 1, 2018 at 8:09pm
David A wrote:

Anyone interested in buying used batteries from phones, laptops and other items from Uganda, please advise on kenninvest@gmail.com

On May 9, 2018 at 2:45pm
Muhammad asim wrote:

I am looking regular used or scrap dry battery supplier in USA my cell 516-728-7942 if you can provide auto batteries in bulk or container load every month

On June 6, 2018 at 3:43pm
MR Idowu wrote:

i have used cell phone batteries for sell. i am from nigeria. i have tested good one. i have the blue and the green result i have up to 135 tons now. please i only need serious buyer to contact me. my cell phone is +2348172597402 am on whatsapp and wechat too. please and please only serious buyer ok

On June 19, 2018 at 12:53am
Mohit Agarwal wrote:

Hi

I am interested in buying used lithium batteries.

Suppliers can contact me from any part of the world.

Thanks.

On June 22, 2018 at 8:33am
Mehrdad Dehghani wrote:

Dear Ms Cardano,

Referring to your message dated April 8th -2018 at Battery University.com forum, We intend to start up a Battery collecting network across the country, from Laptops, Notebooks, Pads, Cellphone, Portable Powertools & toys using rechargeable batteries, and would appreciate it if you inform your more preferred type of batteries for your recycling plant, so that we can collect and store to reach 10-20 tons to ship to you in China.

I would also appreciate it if you indicate an approximate price for your announced preferred batteries in above.

I am on Skype, WhatsApp etc… on +98 912 348 6231

Thank you & Bst Rgds
MD

On July 3, 2018 at 10:50am
MR Idowu wrote:

i am a supplier. you can get back to me on my email or whatsapp akoredesoneye@gmail.com or +2348172597402

On July 19, 2018 at 12:05pm
Samuel wrote:

Hey guys ,am new on this platform,i wanna sell lithuim iron lifepo4 battetries new and dead battery for a cheap price contact @ funnysamuel@gmail.com or via whatsapp +2347034573868

On August 19, 2018 at 8:26pm
General Trading US wrote:

Hey Guys, we are looking for tons of bad/old and unusable auto batteries to purchase at wholesale and if anyone/company has big quantities in USA and Canada please contact us @ generaltradingus@gmail.com and please provide your official company name, website, and phone number as well with detail of your products to see what you have and what are the models, quantities, wholesale price and etc..

On August 23, 2018 at 8:50am
Gonzalo Megarejo wrote:

We have 120 tons for monts battery car used for sale…we are in Chile country. ... covir318@gmail.com

On August 31, 2018 at 7:09am
Shaik Riyazur rahman wrote:

We r purchasing all types of Scrap batterys in Hyderabad
My contact number is:.+91 90520 10000.+91 8309838948

On September 20, 2018 at 3:48pm
Jason Pearce wrote:

Lokesh Tripathi, do you pay 1500 USD per ton of lead acid auto batteries?

On September 21, 2018 at 9:28pm
Sierra metals recycling wrote:

Fatima Susana Martinez Lopez,
Hi we are a battery recycling company based in Raleigh NC and would love to speak with you regarding the possibility of implementing a battery recycling program at your campus as well as partnering with you to purchase the batteries that you collect. Please contact us at sierrametalsrecycling@yahoo.com. Thanks

On September 29, 2018 at 7:08am
Kolapo Ayoola RAJI wrote:

I am just going into battery recycling business in Nigeria . I need a business partner that will provide the equipment and I want to assure you that Nigeria environment is highly conclusive for battery business since the   raw material is in abundant The prospective investor is expected to source for off takers in overseas countries
Any interested investor can please contact me through my e mail address

On October 29, 2018 at 9:48am
serjo wrote:

I’m looking for a buyer of lithium batteries from the cellular industry. My company is located in South America. Be happy to get details from you

Thanks in advance

email :serjo.vh@gmail.com
whatsapp : +972545833004

On October 30, 2018 at 1:20am
Tiger wrote:

we buy end of life mobile and laptop batteries.
kindly whatsapp +.+919082598288

On December 14, 2018 at 11:24pm
vikas patnaik wrote:

hello startups
Am here a consultant and manufacturer
For making lead batteries and solar panels
Like
E rickshaw batteries
Two Wheeler batteries
Inverters batteries
solar panels
For any information contact me
But pls don’t waste time of mine and your self by calling me as a fake .

Thank you


Vikas patnaik
S&B.UC {Solar and Battery unit consultant}
consultant for battery unit setup and solar power unit setup
Business phone no. +91 7027891346
Business gmail id : vikaspatnaik77@gmail.com
Professional linkedin id : vikas patnaik. (entrepreneur investor and CEO at vigorous)
Website : search vigorous batteries

On January 4, 2019 at 12:58am
MOHD RASHID wrote:

Require in bulk quantity spent mobile Lithium ion
batteries for Recycling.
Please contact; 91-7550633477
e-mail; arkrashid20@gmail.com